ASME B16.9 Sib npaug Tee, ASTM A234 WPB, SCH 160
Oct 11, 2025
Dab tsi yog Equal Tee?
Ib qho sib npaug tee yog lub pob tw-weld yeeb nkab haum nrog peb qhov qhib ntawm tib lub npe bore: ob qhov sib npaug kawg ua rau kev khiav, thiab ib ceg txuas ntxiv. Hauv cov kav dej, nws tsim cov ceg sib npaug coj - tawm - ntws ncaj qha los ntawm kev khiav thaum ib feem tswj tau hloov mus los ntawm ceg.
Cov tees sib npaug yog tsim los ntawm kub sib sau los yog txias sib sau los ntawm seamless los yog welded yeeb nkab, ua raws li qhov kawg machining thiab - qhov chaw tsim khoom thiab qib yuav tsum tau nws - ncej- kev kho cua sov (normalizing los yog normalizing- thiab -tempering rau kub-formed {7}fold{7} kev nyuaj siab {2}; fittings thaum teev los ntawm qhov project piping code).
Specification
Khoom npe: Equal Tee
Txuj: ANSI B16.9
Khoom siv: Carbon Steel ASTM A234 WPB
Teem caij: SCH 160
Daim ntawv thov: rau Seamless yeeb nkab
Xaus kev sib txuas: Butt Vuam

Tiv tauj peb rauASTM A234 WPB sib npaug Tee:info@gneepipe.com
Cov qauv siv tau
| Txuj | Title | Dab tsi Nws npog |
|---|---|---|
| ASME B16.9 | Factory-Ua Wrought Butt-Vuam Fittings | Dimensions, kam rau ua, thiab cim rau pob tw -weld fittings NPS 1/2 txog NPS 48. |
| ASTM A234 / A234M ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234M / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234 / ASTM A234) thiab ASTM A234M | Piping Fittings ntawm Wrought Carbon Steel thiab Alloy Steel rau Kev Pabcuam Nruab Nrab thiab Kub Kub | Cov ntaub ntawv xav tau rau qib WPB, WPC, WP1, WP5, WP9, WP11, WP22, thiab WP91. |
| ASME B16.25 | Butt-Vuam xaus | Bevel geometry thiab qhov kawg npaj rau lub pob tw -welding. |
| ASME B36.10 | Welded thiab Seamless Wrought Steel Yeeb Nkab | Phab ntsa-thickness teem sij hawm (SCH 10 txog SCH 160, XXS) thiab cov rooj sib tham OD/phab ntsa. |
Nco tseg ntawm ANSI B16.9:Lub npe "ANSI B16.9" tsis siv lawm. ASME tau ua lub luag haujlwm rau pawg B16 hauv xyoo 1980s. Siv ASME B16.9 ntawm txhua qhov kev yuav khoom tshwj xeeb, cov ntaub ntawv, thiab cov cim cim.
Tshuaj muaj pes tsawg leeg - ASTM A234 WPB
Ladle tsom xam txwv rau ASTM A234 / A234M. Cov khoom tsom xam kam rau ua raws li tus qauv.
| Element | Limit (wt%) |
|---|---|
| Carbon (C), max | 0.30 |
| Manganese (Mn) | 0.29 – 1.06 |
| Phosphorus (P), max | 0.050 |
| Sulfur (S), max | 0.058 |
| Silicon (Si), min | 0.10 |
| Chromium (Cr), max | 0.40 |
| Molybdenum (Mo), max | 0.15 |
| Nickel (Ni), max | 0.40 |
| Copper (Cu), max | 0.40 |
| Vanadium (V), max | 0.08 |
Cov chemistry ntawm A234 WPB yog qhov tseem ceeb sib npaug rau ASTM A106 Qib B seamless yeeb nkab thiab ASTM A53 Qib B. Cov pa roj carbon sib npaug (CE =} C + Mn / {6 +} (Cr + Mo + V) / {5 + (Ni + Cu) / 15 W 4 yam tsis muaj peev xwm zoo. yuav tsum tau preheat nyob rau hauv feem ntau tej yam kev mob.
Mechanical Properties - ASTM A234 WPB
| Khoom | Yam tsawg kawg nkaus |
|---|---|
| Tensile zog | 415 MPa (60,000 psi) |
| Yield zog (0.2% offset) | 240 MPa (35,000 psi) |
| Elongation hauv 2 hauv (50mm) | 22% (ntev ntev); 14% (transverse) |
| Txo thaj tsam, min | 30% |
| Hardness, max | 197 HWB |
Fittings tsim los ntawm phaj (ntau dua li cov yeeb nkab) yuav tsum ua kom tau raws li qhov tsawg kawg nkaus elongation ntawm 17%. Kev ntsuas hardness tsis tas yuav tsum tau tshwj tsis yog tau teev nyob rau hauv daim ntawv xaj yuav khoom.
Siab -Tsuas Muaj Peev Xwm
Ib qho kev nkag siab tsis zoo yog lub pob tw -weld fittings nqa chav kawm siab xws li "Class 300" lossis "PN 64." ASME B16.9 fittings tsis muaj qhov ntsuas qhov siab. Lub peev xwm siab ntawm qhov sib npaug tee yog cov cuab yeej cuab tam - nws nyob ntawm:
- Cov ntaub ntawv tso cai rau kev ntxhov siab (S) ntawm qhov ntsuas kub tsim, ib ASME B31.1 lossis B31.3 Cov Ntawv Ntxiv A
- Phab ntsa thickness ntawm qhov haum kawg (muab rau SCH 160 yeeb nkab)
- Corrosion nyiaj pub dawb thiab zeb undertolerance ntawm qhov project piping class
Raws li ASME B31.3, A234 WPB tau luam tawm cov txiaj ntsig kev ntxhov siab los ntawm −29℃mus rau 425 degree. SCH 160 sib npaug tee nyob rau hauv ib txoj kab B31.3 tsim kom raug tuaj yeem ua haujlwm zoo rau hauv qhov siab - qhov siab ntawm qhov kub nruab nrab. Tib lub tee ntawm 400℃yuav muaj qhov tso cai qis dua - ib txwm suav rau koj txoj cai tswj hwm.
Tswv yim sab sauv txwv:Rau kev pabcuam siab dua 425 degree, hloov mus rau ASTM A234 alloy qib (WP11, WP22, lossis WP91) sib phim rauASTM A335 alloy yeeb nkab. Rau kev pabcuam hauv qab −29 degree, siv ASTM A420 WPL6 (rated rau −46 degree) lossis WPL3 (rated rau −73 degree) hloov WPB.
Kev tiv thaiv saum npoo xws li kub-dip galvanizing (ASTM A153), fusion-bonded epoxy (FBE), los yog peb- txheej polyethylene (3PE) txheej txuas ntxiv kev pab cuam lub neej nyob rau hauv faus, subsea, los yog corrosive - atmosphere daim ntaub ntawv. Txheej tsis hloov lub hauv paus hlau siab ntsuas.
SCH 160 Phab ntsa Thickness - ASME B36.10
Cov lus hauv qab no teev cov phab ntsa nominal thickness rau SCH 160 carbon- steel yeeb nkab rau ASME B36.10. ASME B16.9 xav kom haum phab ntsa thickness tsawg kawg yog sib npaug rau cov phab ntsa nominal ntawm cov yeeb nkab sib txuam.
| NPS | DN | OD (mm) | SCH 160 Phab ntsa (mm) | SCH 160 Phab ntsa (hauv) |
|---|---|---|---|---|
| 1/2 | 15 | 21.3 | 4.78 | 0.188 |
| 3/4 | 20 | 26.7 | 5.56 | 0.219 |
| 1 | 25 | 33.4 | 6.35 | 0.250 |
| 1-1/4 | 32 | 42.2 | 6.35 | 0.250 |
| 1-1/2 | 40 | 48.3 | 7.14 | 0.281 |
| 2 | 50 | 60.3 | 8.74 | 0.344 |
| 2-1/2 | 65 | 73.0 | 9.53 | 0.375 |
| 3 | 80 | 88.9 | 11.13 | 0.438 |
| 4 | 100 | 114.3 | 13.49 | 0.531 |
| 5 | 125 | 141.3 | 15.88 | 0.625 |
| 6 | 150 | 168.3 | 18.26 | 0.719 |
| 8 | 200 | 219.1 | 23.01 | 0.906 |
| 10 | 250 | 273.1 | 28.58 | 1.125 |
| 12 | 300 | 323.9 | 33.32 | 1.312 |
Kho qhov tseem ceeb:NPS 3, 4, thiab 6 SCH 160 phab ntsa thicknesses tau raug txheeb xyuas tawm tsam ASME B36.10. Yav dhau los luam tawm versions ntawm qee lub rooj muaj qhov yuam kev. Ib txwm hla - xyuas nrog ASME B36.10 tsab tam sim no.
Manufacturing thiab Quality Control
tsim
Kub nias los yog txias ua los ntawm seamless yeeb nkab, welded yeeb nkab, los yog phaj. Kub- tsim WPB fittings tau muab rau hauv qhov xwm txheej zoo los kho cov qauv nplej. Txias-tsim fittings tau txais kev ntxhov siab-kev kho cua sov thaum xav tau los ntawm txoj cai kav kav dej.
Tshuab dhos
Lub ntsej muag kawg thiab bevels yog machined rau ASME B16.25 (37.5℃± 2.5℃bevel nrog 1.6 hli ± 0.8 hli hauv paus lub ntsej muag). Ceg thiab khiav bores raug txheeb xyuas nrog go/no-go gauges.
Kev tshuaj xyuas thiab kuaj
- Dimensional soj ntsuam - 100% ntawm fittings los yog ib qho qauv qauv pom zoo nrog tus neeg yuav khoom
- Hydrostatic test - thaum teev nyob rau ntawm daim ntawv yuav khoom
- Tsis yog -kev kuaj xyuas kev puas tsuaj (RT / UT / MT / PT) - ib qhov project specification
- Tensile xeem - ib qho cua sov lossis ntau rau ASTM A234
- Tshuaj ntsuam xyuas - ladle tsom xam rau ib lub tshav kub
Kos npe
Txhua qhov haum yuav tsum raug cim nrog cov chaw tsim khoom lub npe lossis cov cim lag luam, qib khoom siv (WPB), tus qauv loj (B16.9), lub npe loj thiab lub sijhawm, tus lej kub lossis ntau tus lej.
Daim ntawv thov
- Fais fab nroj tsuag - lub ntsiab chav dej, feedwater, blowdown, thiab condensate kab.
- Roj thiab roj - sib sau cov kab, xa cov kav dej, thiab txheej txheem kav.
- Tshuaj thiab petrochemical - txheej txheem thiab cov kav dej siv hluav taws xob.
- Refineries - refinery off-ploj thiab interconnecting piping.
- Shipbuilding thiab offshore platforms - ballast, bilge, firewater, thiab utility systems.
Tsis pom zoo rau kev faib dej tsis kho, faus dej hauv cov dej tsis muaj txheej, lossis cov kev pabcuam uas cov kua dej corrosivity ntau dua li cov pa roj carbon steel tsis muaj peev xwm.
Daim ntawv txheeb xyuas khoom
- Qhia meej ASME B16.9 hloov tsis tau ANSI B16.9.
- Qhia meej ASTM A234 Qib WPB cov khoom.
- Xeev NPS/DN thiab phab ntsa (SCH 160).
- Qhia lub pob tw -weld bevels rau ASME B16.25.
- Yuav tsum tau EN 10204 Hom 3.1 cov ntaub ntawv xeem ntawv pov thawj.
- Rau kev pabcuam qaub, ntxiv NACE MR0175 / ISO 15156 ua raws.
- Rau qhov qis - qhov kev pabcuam kub, qhia txog Charpy qhov kev sim cuam tshuam.
- Rau corrosive ib puag ncig, qhia cov txheej txheem txheej txheej.
FAQs
Q1: Dab tsi yog qhov txawv ntawm qhov sib npaug tee thiab txo tee?
Ib qho sib npaug tee muaj peb qhov qhib ntawm tib lub npe loj; ib tug txo tee muaj ib ceg me me bore. Siv ib qho sib npaug tee thaum ceg kab nqa tag nrho kab loj.
Q2: Puas tuaj yeem ASTM A234 WPB sib npaug tees siv thaum kub hauv qab -29 degree?
Tsis yog tsis muaj kev tsim nyog. Hauv qab −29 degree, kev ntsuam xyuas cuam tshuam yuav tsum tau ua raws li ASME B31.3 qis-cov cai ntsuas kub. Lwm cov ntaub ntawv suav nrog ASTM A420 WPL6 lossis WPL3.
Q3: SCH 160 txhais li cas?
SCH 160 yog phab ntsa -thickness designation hauv ASME B36.10. Nws yog qhov hnyav- phab ntsa tuab dua SCH 80 thiab SCH 40.
Q4: Puas yog seamless lossis welded sib npaug tee zoo dua?
Ob txoj kev tsim khoom tuaj yeem ua raws li ASME B16.9 thaum tsim khoom kom raug, cua sov- kho, thiab tshuaj xyuas. Kev xaiv nyob ntawm qhov project xav tau, muaj, thiab tus nqi.
Q5: Dab tsi yog qhov ntsuas siab ntawm SCH 160 sib npaug tee?
ASME B16.9 fittings tsis nqa qhov ntsuas siab ruaj khov. Lub peev xwm siab yuav tsum raug xam raws li cov khoom siv kev ntxhov siab, qhov kub thiab txias, phab ntsa thickness, thiab cov kav dej siv tau.
Cov ntaub ntawv
- ASME B16.9 - Factory-Made Wrought Butt-Vuam Fittings
- ASTM A234 / A234M - Txuj Specification rau Piping Fittings ntawm Wrought Carbon Steel thiab Alloy Steel
- ASME B36.10 - Welded thiab Seamless Wrought Steel Yeeb Nkab
- ASME B31.3 - Txheej Txheem Piping
- ASME B16.25 - Butt-Vuam xaus
- NACE MR0175 / ISO 15156 - Cov ntaub ntawv siv rau hauv H₂S-Containing Environments