ASTM A269 TP316H Stainless Hlau Seamless Tubes
Oct 30, 2023
TP316H yog lub siab carbon version ntawm TP316, uas yog qib austenitic stainless hlau. TP316H muaj cov ntsiab lus ntawm cov pa roj carbon ntau dua li TP316, uas txhim kho nws lub zog kub thiab corrosion kuj.
ASTM A269 TP 316H Cov Lus Qhiacov raj yuav tsum tau ua kom tau raws li cov khoom siv tshwj xeeb, xws li lub zog tensile, yield zog, thiab elongation, kom ntseeg tau tias lawv tuaj yeem ua tau zoo nyob rau hauv qhov kub thiab txias.
Cov txheej txheem suav nrog ntau yam kev ntsuam xyuas kom ntseeg tau tias cov raj zoo, suav nrog kev sim tsis muaj kev puas tsuaj, kev sim hydrostatic, thiab kev ntsuas tam sim no.
Daim ntawv thov: ASTM A269 TP316H stainless hlau seamless hlab yog feem ntau siv nyob rau hauv kev lag luam uas yuav tsum tau high-temperature thiab high-corrosion kuj. Qhov no tuaj yeem suav nrog kev siv tshuaj lom neeg, petrochemical, thiab kev lag luam tshuaj.

Tshuaj muaj pes tsawg leeg ntawm ASTM A269 TP316H Stainless Hlau Seamless Tubes
| Qib | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 316 | Min | - | - | - | 0 | - | 16.0 | 2.00 | 10.0 | - |
| Max | 0.08 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.10 | |
| 316L | Min | - | - | - | - | - | 16.0 | 2.00 | 10.0 | - |
| Max | 0.03 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.10 | |
| 316H | Min | 0.04 | 0.04 | 0 | - | - | 16.0 | 2.00 | 10.0 | - |
| max | 0.10 | 0.10 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | - |
Mechanical Properties ntawm ASTM A269 TP316H Stainless Hlau Seamless Tubes
| Qib | Tensile Str (MPa) min |
Yield Str 0.2% Pov thawj (MPa) min |
Elong (% hauv 50mm) min |
Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 316 | 515 | 205 | 40 | 95 | 217 |
| 316L | 485 | 170 | 40 | 95 | 217 |
| 316H | 515 | 205 | 40 | 95 | 217 |
ASTM A269 TP316H Stainless Hlau Seamless Tubes Lub cev muaj zog
| Qib | Qhov ntom (kg / m3) |
Elastic Modulus (GPa) |
Lub ntsiab lus sib xyaw ua ke ntawm Thermal Expansion (µm / m / degree) | Thermal conductivity (W/m.K) |
Tshwj xeeb kub 0-100 degree (J/kg.K) |
Elec Resistivity (nΩ.m) |
|||
| 0-100 degree | 0-315 degree | 0-538 degree | Ntawm 100 degree | Ntawm 500 degree | |||||
| 316/L/H | 8000 | 193 | 15.9 | 16.2 | 17.5 | 16.3 | 21.5 | 500 | 740 |
Qib Specification Sib piv rau ASTM A269 TP316L Stainless Hlau Seamless Tubes
| Qib | UNS No | Laus British | Euronorm | Swedish SS |
Nyiv JIS |
||
| BS | En | Tsis muaj | Lub npe | ||||
| 316 | S31600 | 316S31 | 58H, 58J | 1.4401 | X5CrNiMo17-12-2 | 2347 | TIAB SA 316 |
| 316L | S31603 | 316S11 | - | 1.4404 | X2CrNiMo17-12-2 | 2348 | SUS 316L |
| 316H | S31609 | 316S51 | - | - | - | - | - |