ASTM A335 Qib P22 Alloy Steel Yeeb Rau Boiler thiab superheater

Nov 06, 2025

Dab tsi yog ASTM A335?

ASME SA335 / ASTM A335, chrome - moly ferritic alloy {} Cov yeeb nkab sib xyaw ua ke rau cov kev pabcuam kub. Cov yeeb nkab xaj rau qhov kev cai tshwj xeeb no yuav tsum tsim nyog rau kev khoov, flanging, zoo ib yam kev ua haujlwm thiab rau kev sib tw ua ke vuam.

 

P22 cov khoom siv yog dab tsi?

A335 / sa335 Qib P22 Alloy Steel Seamless kav yog cov roj carbon steel pipes nrog ntxiv ntawm chromium, molybdenum, thiab qee zaum vanadium. Chromium, lossis chrome, txhim kho siab- kub lub zog, nce oxidation ua kom zoo thiab seb puas thiab hardness hauv chav sov.

 

ASTM A335 P22 Seamless Alloy Steel Boiler Kav

Lub hom phiaj ASTM A335 P22, SA335 P22
Qhov loj 1/2"- 24"
Lub luag haujlwm Sch.10 rau Sch.XXS
Ntaus Seamless / Erw / Welded / Fabricated
Qho ntev Ib leeg random, ob npaug random & txiav ntev
A335 P22 Yeeb Nkab Tiaj kawg, beveled kawg, tsuj las
Kev siv Seamless Ferritic Alloy - steel yeeb nkab rau high-}} kub kev pab

 

A335 P22 Alloy Steel Seamless Tube rau qhov kub siv hluav taws xob kev ntsuas tshuaj max%

Teem nqi Pa roj carbon Tus kws dai txiv manganese Phosphorus Leej mos Silicon Yeebsab Molybdenum
P22 0.05-0.15 0.3-0.6 0.025 0.025 0.5 1.9-2.6 0.87-1.13

 

ASTM A335 P22 Alloy Hlau Seamless Tubes Kub dov rau Boiler Neeg Kho Tshuab

Teem nqi Yield zog (mpa) Tensile lub zog (mpa) Elongation (%) High - lub zog kub
P22 0.05-0.15 0.3-0.6 0.025 Nyob zoo txog 593℃(1100℃f)

 

ASTM A335 P22 Alloy Steel Seamless Yeeb Nkab Yeeb Nkab Xim Beveled Sib Xws Li Cov Khoom Sib Xws

ASTM ASME Khoom siv sib npaug JIS G 3458 Tsis yog Bs Din ISO Abs Tus leeg Lrs
A335 P22 SA335 P22 T22, 10CRMO910, 10CRMO9-10, 1.7380, 11CRMO9-10, 1.7383 Stpa 24 K21590 3604 P1 622 17175 10} crmo910 2604 II TS34 ABS 13 KSTPA 24 SEC 22-1 / 4CR1MO410

 

Sab nraud txoj kab uas hla sab nraud ntawm Astm A335

Nps (DN) Tus Tsim Qauv Saum Hauv qab
nyob rau hauv. lub hli nyob rau hauv. lub hli
1/8 rau 1 1 / 2 (6 txog 40), incl. 1/64(0.015) 0.40 1/64(0.015) 0.40
Tshaj 1 1 / 2 mus rau 4 (40 mus rau 100), incl 1//32(0.031) 0.79 1/32(0.031) 0.79
Tshaj 4 txog 8 (100 rau 200), incl. 1/16(0.062) 1.59 1/32(0.031) 0.79

Tshaj 8 txog 12 (200 txog 300), incl.

3/32(0.093) 2.38 1/32(0.031) 0.79

 

Yuav Tsum Tau Ceev

Teem nqi Hom Kev Kho Sov Normalizing qhov ntsuas kub f [c] Subcritical annealing los yog tempering kub ntau yam f [c]
P22 Tag nrho los yog isothermal anneal    
  Normalize thiab npau taws   1250 [675]

 

Kev ua siab ntev rau Astm A335 / ASME SA 33-4 P22 Seamless kav

Nps Of thev Nps Wht kam rau
1/8 "Tsawg dua lossis sib luag rau NPS tsawg dua lossis sib npaug rau 1 1 / 2" +/- 0.4 1/8 "Tsawg dua lossis sib npaug ntawm NPS tsawg dua lossis sib npaug rau 2 1 / 2", txhua tus T / D qhov sib piv. +20%, -12.5%
{{01 1 / 2 +/- 0.79 Nps ntau dua los yog sib npaug rau 2 1 / 2 ", t / d tsawg dua los yog sib npaug rau 5% +22.5%, -12.5%
4 " +1.59, -0.79 Nps ntau dua los yog sib npaug rau 2 1 / 2 ", T / D> 5% +15%, -12.5%
8 " +2.38, -0.79 (T=teev phab ntsa tuab; d=teev sab nraud ntawm lub taub)
Nps> 12 " +/- 1%

 

Daim ntawv thov Astm A335 P22

1.Txhua siv tiam: Nws yog dav siv nyob rau hauv cov nroj tsuag fais fab rau kev tsim cov boiles boiles, chav head, thiab trave supereater / mam li rov qab. Lub Alloy Steel sib xyaw ntawm P22 tau muab qhov tseem ceeb tshaj plaws rau cov kub thiab xeb, ua rau nws haum rau cov khoom tseem ceeb no.

2. Tsis txhob siv cov A335 P225 P225 P225 P225 P225 P225 P222 yog siv rau kev tsim kho cov kav dej thiab cov fittings rau cov roj thiab roj ua kom dawb. Nws yog tshwj xeeb tsim los tiv thaiv cov roj av ua kom zoo nkauj, suav nrog kev kub siab, thiab cov ntawv thov siab.

3. Dememical Ua: P22 Alloy Steel Kave yog siv rau hauv cov nroj tsuag ua noj rau ntau yam kev siv, suav nrog cov tshuaj ua kua thiab raug cov cua sov. Nws txoj kev tawm tsam rau oxidation thiab corrosion ua rau nws haum rau kev tuav ntau cov tshuaj lom neeg.

4.Petrochemical kev lag luam: P22 kav nrhiav cov kev lag luam petrochemical dav rau kev thauj khoom ntawm cov tshuaj lom neeg, roj av, thiab hydrocarbons ntawm qhov kub thiab kub. Lawv feem ntau ua haujlwm hauv kev tsim kho cov hlab ntsha ua kom sov, kev hloov pauv kub, thiab lwm yam khoom tseem ceeb.

 