Qhov sib txawv ntawm 2205 steel thiab 2507 steel
Oct 25, 2024
2205 yog ib tug duplex stainless hlau thiab 2507 yog ib tug super duplex stainless hlau.
Cov khoom tseem ceeb ntawm 2205 duplex steel yog chromium, npib tsib xee, thiab nitrogen, uas cov ntsiab lus ntawm chromium yog li 22%, cov ntsiab lus ntawm npib tsib xee yog li 5%, thiab cov ntsiab lus ntawm nitrogen yog li 3%.
Cov ntsiab lus ntawm nickel yog li 5%, cov ntsiab lus yog li 3%, thiab cov ntsiab lus ntawm nitrogen yog li ntawm 0.18%.
Cov khoom tseem ceeb ntawm 2507 duplex steel yog chromium, npib tsib xee, thiab tooj liab, uas cov ntsiab lus ntawm chromium yog li 25%.
Cov ntsiab lus ntawm npib tsib xee yog li 7%, cov ntsiab lus ntawm cov nyiaj yog li 4%, thiab cov ntsiab lus ntawm tooj liab yog li ntawm 0.5%.
Lub zog tensile ntawm 2205 duplex steel yog hais txog 620 MPA, lub zog tawm los yog li 450 MPA, thiab elongation yog li 25%.
2507 duplex steel muaj lub zog tensile ntawm kwv yees li 800 MPA, lub zog tawm ntawm kwv yees li 550 MPA thiab elongation ntawm kwv yees li 25%.

2205 duplex steel muaj kev tiv thaiv corrosion zoo heev thiab tuaj yeem siv rau hauv ntau yam corrosive media, nrog rau cov kua qaub, alkalis thiab ntsev. Nws tsis kam mus rau chloride kev nyuaj siab corrosion yog superior rau ntawm ib txwm austenitic stainless hlau.
2507 duplex steel muaj ntau dua corrosion kuj, tshwj xeeb tshaj yog nyob rau hauv chloride-muaj xov xwm. Nws cov chloride kev nyuaj siab corrosion kuj yog hais txog ob zaug siab li 2205 duplex steel, uas tuaj yeem ua tau raws li kev siv ntau dua.

Vim nws lub zog siab thiab siab corrosion kuj, 2507 stainless hlau yog tsuas yog siv nyob rau hauv chemical kev lag luam, roj thiab roj extraction, marine engineering thiab kub kub thiab kub siab ib puag ncig, thiab lwm yam. 2205 stainless hlau yog dav siv nyob rau hauv lub teb ntawm architectural kho kom zoo nkauj, kev ua zaub mov thiab khoom siv kho mob vim nws tus nqi qis dua thiab zoo dua corrosion kuj.