Qhov sib txawv ntawm kev ua kom huv si pob li qub thiab muaj kev muaj cuab yeej sib npaug
Aug 14, 2025
Huv -} qib pob li qub xa mus rau li qub ua los ntawm304ss lossis 316 Stainless hlau, FeaturingCov Qauv Hluav Taws XobCov. Lawv cov chaw du ua kom huv si, tshem tawm cov chaw sib txuas lus, thiab tiv thaiv cov peev xwm tshwj xeeb rau ntau yam hauv cov zaub mov, biopharmaceutical, thiab lwm daim teb. Tus du, seamless, thiab tus kheej- Cov kua dej ntws tawm kuj tseem ua rau lawv haum rau {}} qhov chaw (SIP) tu. Txoj kev sib txuas rau cov khoom huv, flanged, welded, clamp, thiab ferrule hom, xaiv raws li cov kev qhia tshwj xeeb. Cov kev sib txawv ntawm cov li qub thiab cov khoom siv khoom lag luam li qub yog li nram no:
1. Valve lub cev cov khoom siv
Huv Si Pob Li QubTshwj siv siv304ss, 304L, 316, lossis 316L Stainless hlauCov. Tom qab tsim khoom, lawv raug kev kho tshwj xeeb.
Kev siv li qubSiv cov ntaub ntawv xws li cam khwb cia hlau, cov hlau cam khwb cia, zas, thiab hlau stainless, thiab stainless hlau, muab ib qho kev xaiv dav dav.
Huv li qub yog siv nyob rau hauv ib puag ncig nrog txoj hlua kev sib cav sib haum (xws li cov tshuaj, khoom noj, cov khoom lag luam txhua hnub), nyob qhov twg hu rau tib neeg lub cev. Yog li no, kev tsim khoom ntau lawm yuav tsum tau ua kom tiav cov qauv kev huv. Cov Khoom Siv Hluav Taws Xob (steel, hlau, tooj liab) ua tsis tau raws li cov kev xav tau no:
Hlau Thiab Hlau Li QubCorrode thiab xeb nyob rau hauv high - av noo kua lossis huab cua, cov khoom lag luam.
Tooj liab li qubZoo sib xws corrode, thiab cov txiaj ntsig verdigris(Toxic Tooj Liab Patina)Yog qhov tsis haum rau kev siv cov ntawv thov huv huv.

2. Tsos
Huv Si Pob Li QubYam zooTxheem electropolished chaw, Ua kom huv si yam tsis muaj zog yam tsis muaj xov xwm tawm suab lossis muaj peev xwm sib kis.
Kev siv li qubFeem ntau tau tsim raws li kev xav tau ua haujlwm, ua ntej ntev hauv high {{} {{{{}}}}}} kev hloov kho tau. Lawv cov tsos thiab sab hauv tsis tshua du thiab ua kom zoo dua li cov li qub, tab sis lawv nyob twj ywm irreplacable hauv ntau daim ntawv thov.
3. Kev Txuas Txuas
Huv Si Pob Li QubFeem ntau sivclamp (sai - Txuas) lossis xov txuas txuas.
Kev siv li qubNtiavFlanged, xov xwm ceev, nrawm-} Txuas, welded, lossis lwm yam sib txuas.
Piv txwv li, tusVONT VONY TXHAJ HUV Pob Valve (USA)Cov khoom ua pov thawj cov hauv qab no cov hauv kev lag luam li qub:
Lub valve khoom: 304 lossis 316L stainless hlau (xov xwm - kev sib tiv tauj thaj chaw).
Daim ntsaws ruaj ruaj: Lub zog tiv taus rau cov acids, alkalis, thiab kub siab.
Kev sib txuas: Welded, sai - Txuas, lossis hom xov tooj.
Zoo heev: Sab hauv thiab sab nraud thaj chaw polished kom tau raws li cov qauv precision.
Kev nplig: Nruj me ntsis ua raws li 3a, din, SMS, BS, thiab lwm yam qauv zam.
Ua Haujlwm Siab: 1.0 MPA.
Tsev hauj lwm kub: -10℃rau +150 degree.
Foob cov ntaub ntawv: PTFE (feem ntau yog hu ua Teflon), Txheem EPDM, nrog silicone lossis fluororubber Lwm muaj.
Xov Xwm Tshaj: Kua, roj av, roj, thiab cov tshuaj corrosive heev.