Dab tsi yog cov khoom sib npaug ntawm A335 p5 alloy yeeb nkab

Jul 02, 2025

1. Cov qauv sib luag thoob ntiaj teb

Lub teb chaws Lub hom phiaj Teem nqi Kev cim
U‌.S. ASTM A335 \/ A335M Qib P5 Yooj yim siab kub Alloy Cov Khoom Siv Hluav Taws Xob
U.S. ASME SA -335 Qib P5 Cov Qauv Sib Tham Tshwj Xeeb Rau Cov Khoom Siv Siab
European Union En 10216-2 15crro5 Meej lawm cov khoom xyaw thiab kev ua tau zoo
Nyiaj txiag JIS G3467 Stpa 25 Kev kwv yees CR-MO system cua sov-resistant hlau

2. Nqe lus sib npaug

Lub teb chaws Teem nqi

Tshuaj Muaj Tshuaj

Cov Ntawv Thov
Ntau lub teb chaws 5Cl -0. 5mo 5% cr -0. 5% mo Cov Cim Txhab Rau Cov Ntsuas Kub Siab Kev Kub Siab
European Union X3crmo5 4. {{{0 - 3. {}}}}}}. 45 - 0. 65% mo Sib npaug rau en 15crmo5
U‌.S.A. T5(Kev Zam Txim \/ Castings) Tib yam khoom xyaw ua p5 ASME BOILER COMPITE Ntxiv Thov
Nyiaj txiag Suh5 5% cr -0. 5% mo Kwv yees cov qhab nia ntawm cov hlau ua cua sov-resistant

3. Cov yam ntxwv tseem ceeb thiab cov khoom siv ntawm daim ntawv thov
Qhov kub thiab txias yoog raws li 450-600 degree (qee cov tub ntxhais kawm muaj kev txwv siab tshaj plaws ntawm 650 degree yuav tsum tau raws li kev pom zoo nrog kev ceev faj);
Cov kev ua tau zoo: Kev kub siab rau lub zog los tiv thaiv kev tiv thaiv hydrogen txheej (petrochemical hydrogenation chav nyob)

A335 P11 alloy pipe for high temperature