Stainless hlau 304H cov kav dej
Oct 19, 2023
Dab tsi yog 304h stainless hlau yeeb nkab?
304H stainless hlauyog lub siab carbon version ntawm 304 stainless hlau alloy. Nws yog tsim los muab kev txhim kho qhov kub thiab txias zog thiab nkag tau zoo dua piv rau cov qauv 304 alloys. 304H stainless hlau yeeb nkab feem ntau yog siv nyob rau hauv high-temperature daim ntaub ntawv xws li nyob rau hauv petrochemical, tshuaj, thiab fais fab kev lag luam.
Dab tsi yog kev siv ntawm Stainless Hlau 304H Pipes?
Stainless hlau 304H kav dej yog siv nyob rau hauv high-temperature daim ntaub ntawv xws li nyob rau hauv petrochemical, tshuaj, thiab hluav taws xob kev lag luam. Lawv kuj tseem siv rau hauv boilers, kub exchangers, thiab lwm yam high-temperature daim ntaub ntawv uas corrosion kuj thiab high-temperature zog yog qhov tseem ceeb. Tsis tas li ntawd, 304H cov kav dej tau siv rau hauv kev ua zaub mov thiab kev lag luam khoom noj siv mis vim lawv tsis kam tiv thaiv corrosion thiab muaj peev xwm los ntxuav tau yooj yim.
Stainless hlau 304H Tubes & Tubes sib npaug qib
| STANDARD | WERKSTOFF NR. | UNS | JIS | AFNOR | BS | GOST | EN |
| SIB 304H | 1.4301 | S30409 | – | – | – | – | – |
TP 304H Stainless Hlau Yeeb Nkab & Tubes Chemical Composition:
| Qib | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 304H | min. | 0.04 | – | – | – | – | 18.0 | – | 8.0 | – |
| max. | 0.10 | 2.0 | 0.75 | 0.045 | 0.030 | 20.0 | 10.5 | |||
Lub cev muaj zog:
| Qib | Qhov ceev (kg / m3) | Elastic Modulus (GPa) | Mean Coefficient ntawm Thermal Expansion (m/m/0C) | Thermal conductivity (W / mK) | Kub tshwj xeeb 0-1000C (J/kg.K) | Hluav taws xob tiv taus (nm) | |||
| 0-1000C | 0-3150C | 0-5380C | ntawm 1000C | ntawm 5000C | |||||
| 304H | 8000 | 193 | 17.2 | 17.8 | 18.4 | 16.2 | 21.5 | 500 | 720 |

Lub tuam txhab kom zoo dua
Peb muab cov qauv dawb xwb, tab sis cov khoom thauj yuav tsum tau them los ntawm tus neeg yuav khoom.Peb muaj cov khoom lag luam tag nrho, thiab tuaj yeem xa tuaj tsis pub dhau lub sijhawm luv. Ntau yam rau koj xaiv. OEM thiab ODM kev txiav txim raug lees txais, Txhua yam ntawm lub logo luam tawm lossis tsim muaj.Zoo Zoo + Lub Hoobkas Nqe + Cov Lus Teb Ceev + Kev Pabcuam Zoo, yog qhov peb sim ua kom zoo tshaj plaws rau koj.