Dab tsi yog qhov txawv ntawm 45 # steel thiab Q235?
1. Tus naj npawb steel yog qhia nyob rau hauv ntau txoj kev. No. 45 steel qhia cov tshuaj muaj pes tsawg leeg ntawm cov hlau. Qhov nruab nrab carbon cov ntsiab lus ntawm cov hlau no yog 0.45%, yog li nws hu ua No. 45 steel.Q235steel sawv cev rau txhua yam khoom ntawm hlau. Q nyob rau hauv tus lej steel sawv cev lub zog tawm los

2. Cov ntsiab lus carbon thiab kev siv sib txawv. No. 45 steel muaj cov ntsiab lus carbon ntawm 45/10, 000 thiab yog cov khoom siv hlau. Q235 muaj cov ntsiab lus carbon tsawg dua 20/10, 000 thiab yog cov hlau engineering.

3. Cov khoom sib txawv. 45 steel yog nruab nrab carbon steel thiab tuaj yeem tua tau. Nws muaj lub zog siab thiab hardness tom qab kev kho cua sov thiab tsim nyog rau kev ua cov khoom siv kho tshuab. Q235 steel yog ib hom qis carbon steel nrog siab plasticity tab sis tsis muaj zog. Nws yog tsim rau kev kos duab thiab dov ua.