Dab tsi yog SA 210 cov khoom siv yeeb nkab
Mar 27, 2024
- ASTM A210 / ASME SA210 specifications npog seamless nruab nrab carbon steel boiler hlab thiab superheater raj. Cov lus qhia tshwj xeeb kuj hais txog qhov tsawg kawg nkaus ntawm phab ntsa thickness, steel tube qhov ntev, boiler flues (nrog rau kev nyab xeeb kawg), arched tubes thiab dwell tubes. Cov lus qhia tshwj xeeb muab cov khoom tensile thiab hardness, tab sis tsuas yog nyob rau hauv qee qhov kev txwv. Cov ntaub ntawv yuav tsum tau ua los ntawm kev tua. Cov kav hlau yuav tsum tau tsim los siv cov txheej txheem seamless thiab cim tias ua haujlwm kub lossis txias. Qhov saum npoo yuav tsum tau hais meej meej ntawm qhov kev txiav txim. Cov tshuaj muaj pes tsawg leeg yuav tsum ua tau raws li qhov yuav tsum tau ua. Kev siv cov khoom xyaw tseem ceeb tshaj li cov npe ntawm no tsis tso cai. Cov qauv yuav tsum raug kuaj tensile, flattening test, expansion test, hardness test, hydraulic test los yog non-destructive electronic test. Superheater raj yuav tsum tau tsim yam tsis muaj qhov tsis xws luag thiab muaj peev xwm tiv thaiv kev nthuav dav, crease, forging, vuam thiab khoov.
-
ASTM A210 / ASME SA210 Boiler Tube
Mechanical Properties:
| Qib | C (Max) | Mn | Si (Min) | P (Max) | S (Max) |
| A1 | 0.27 | Max 0.93 | 0.1 | 0.035 | 0.035 |
| C | 0.35 | 0.29~1.06 | 0.1 | 0.035 | 0.035 |
Tshuaj muaj pes tsawg leeg ntawm A210 Carbon Steel Seamless Tube:
| Qib | Tensile zog (Mpa) | Yield zog (Mpa) | Elongation (%) |
| A1 | Ntau dua lossis sib npaug rau 415 | Ntau dua lossis sib npaug li 255 | Ntau tshaj los yog sib npaug rau 30 |
| C | Ntau dua lossis sib npaug rau 485 | Ntau dua lossis sib npaug li 275 | Ntau tshaj los yog sib npaug rau 30 |
Sab nraud txoj kab uas hla & kam rau ua ntawm SA210 Boiler Flue Pipe
| Txheej txheem | Sab nraud txoj kab uas hla, mm | Kev kam rau siab,% |
| Kub dov | OD Tsawg dua lossis sib npaug rau 101.6 | -0.5 |
| 101.6<OD Tsawg dua lossis sib npaug rau 127 | -0.333333333 | |
| Txias Drawn | OD 25.4 | ±0.10 |
| 25.4 Tsawg dua lossis sib npaug rau OD Tsawg dua lossis sib npaug rau 38.1 | ±0.15 | |
| 38.1 OD 50.8 | ±0.20 | |
| 50.8 Tsawg dua lossis sib npaug rau OD<63.5 | ±0.25 | |
| 63.5 Tsawg dua lossis sib npaug rau OD<76.2 | ±0.30 | |
| 76.2 Tsawg dua lossis sib npaug rau OD Tsawg dua lossis sib npaug rau 101.6 | ±0.38 | |
| 101.6<OD Tsawg dua lossis sib npaug rau 127 | -0.59375 |
GNEE Group yog tshwj xeeb hauv kev muab A210 / SA210 boiler raj, txias drawn tubes, thiab kub dov raj, koj txais tos raunugthaum twg los tau.