Cov khoom siv SA 213 T91 yog dab tsi
Jan 06, 2026
T91 seamless steel yeeb nkab, tseem hu ua 9Cr-1Mo steel, yog hloov kho 9Cr-1MoVNb steel. Cov hlau no muaj cov tshuaj ua kom zoo; los ntawm kev ntxiv cov kab ntawm vanadium (V) thiab niobium (Nb), nws qhov kub-kub creep zog thiab endurance lub zog yog ho txhim kho. Ib txhij, T91 seamless steel yeeb nkab kuj muaj oxidation zoo heev thiab corrosion kuj, tswj kev ua haujlwm ruaj khov nyob rau hauv ib puag ncig hnyav xws li kub thiab kub siab.
Tshuaj muaj pes tsawg leeg ntawm T91 Steel (%)
Lub ntsiab lus
C 0.08-0.12
0.30-0.60 Nws
P Tsawg dua lossis sib npaug li 0.02
S Tsawg dua los yog sib npaug rau 0.01
0.20-0.50 Nws
8.00-9.50 Nws
0.85-1.05 Nws
V 0.18-0.25
Ib 0.06-0.10
N 0.03-0.07
Ni Tsawg dua lossis sib npaug li 0.40
Daim ntawv thov:
1. Fais Fab Boiler Systems: Qhov no yog thawj daim ntawv thov ntawm T91 alloy tubing. Nyob rau hauv niaj hnub thermal fais fab nroj tsuag boilers ua hauj lwm nyob rau hauv high kub thiab pressures, xws li superheater thiab reheater piping, kub tuaj yeem ncav cuag ntau pua degrees Celsius thiab siab heev. T91 tubing tuaj yeem tiv taus cov xwm txheej huab cua no thiab yog ib feem tseem ceeb rau kev txhim kho boiler efficiency thiab ua kom muaj kev nyab xeeb thiab kev lag luam ntawm lub tshuab fais fab.
2. Petrochemical Equipment: T91 alloy tubing kuj plays lub luag hauj lwm nyob rau hauv siab - kub exchangers thiab reformer piping nyob rau hauv ib co roj refining thiab tshuaj nroj tsuag, withstanding siab - kub txheej txheem xov xwm.
3. Lwm yam High -Tsuas Kub thiab Siab- Cov Yeeb Nkab Siab: Hauv qee qhov tshwj xeeb muaj cov kav dej uas xav tau kev tiv thaiv siab - qhov kub thiab txias, qhov chaw ua haujlwm txwv qhov kev ua tau zoo ntawm cov khoom siv zoo tib yam, T91 alloy tubing yog qhov kev xaiv zoo.
A213 T91 kub exchanger raj hauv Tshuag