T92 alloy steel yeeb nkab, tseem hu ua T92 alloy seamless steel yeeb nkab, yog martensitic cua sov-resistant steel raws li American ASTM tus qauv. Cov yeeb nkab steel no muaj 8.5%-9.5% chromium, 0.3%-0.6% molybdenum, thiab cov khoom alloying xws li tungsten, vanadium, thiab niobium. Nws qhov kev khiav hauj lwm kub tuaj yeem ncav cuag 650 degree, thiab nws yog siv rau hauv superheaters, reheater tubes, thiab cov kav dej tseem ceeb ntawm cov boilers ultra-supercritical boilers, nrog rau cov khoom kub kub hauv nuclear fais fab nroj tsuag.

GNEE Group tshwj xeeb hauv kev muab cov raj xa dej boiler, yog ASTM tau ntawv pov thawj, thiab muaj cov kev pabcuam steel yeeb nkab. covXav tau siab -cov kav hlau zoo rau koj qhov project? Nug tam sim no thiab txaus siab rau lub neej warranty!

 

 

ASME SA213 T92 Alloy Steel Seamless Tubing Chemical Composition

P, % S, % Si,% Tsis yog,% W, % B, % Al,% Nb,% Cr,% Mo,% V, % C, % Mn,% N, %
0.02 max 0.01 max Max 0.5 hli 0.4 max 1.5-2.0 0.001-0.006 0.04 max 0.04-0.09 8.5-9.5 0.3-0.6 0.15-0.25 0.07-0.13 0.3-0.6 0.03-0.07

 

SA213 T92 Seamless Tube Mechanical Properties

Yield zog, MPa Tensile zog, MPa Hardness, HB Elongation,%
440 yam tsawg kawg nkaus 620 yam tsawg kawg nkaus 250 qhov siab tshaj plaws 20 yam tsawg kawg nkaus

‌

A213 T92 Khoom Specification

Qib Alloy Steel A335 GR P92 / AS A213 GR T92
Xaus Plain, Beveled, Treaded
Specification ASTM A213 A335 / ASME SA213, SA335
Loj 1/2 nti NB - 24 nti NB
Daim ntawv Square, Round, Hydraulic, Rectangular thiab lwm yam
Ntev Ib Leeg, Ob Chav & Txiav Ntev.
Thickness SCH20, SCH160, XXS XS, SCH80, SCH60, SCH140, SCH120, SCH80, SCH40, SCH30, STD,
Hom ERW / Seamless / Fabricated / Welded / LSAW Pipes

 

Piv rau cov kav dej seamless steel zoo tib yam, T92 qhov zoo tshaj plaws yog:

1. High -kub stability: Los ntawm nano- theem MX carbonitride nag lossis daus, cov khoom nkag rupture lub neej ntawm 600-650℃yog nce ntau tshaj 3 zaug;

2. Optimized weldability: Nrog rau cov pa sib npaug (CE) tsawg dua lossis sib npaug li 0.25%, ua ke nrog tom qab-weld kev kho cua sov, txias tawg tuaj yeem zam tau zoo;

3. Kev hloov pauv kev lag luam: Raws li tib yam kev ua haujlwm, phab ntsa tuab tuaj yeem txo tau 30% piv rau austenitic steels xws li TP347H, txo cov khoom hnyav thiab tus nqi.

 

SA213 T92 seamless yeeb nkab Ntau lawm txheej txheem thiab kev sib tw

SA213T92 seamless steel yeeb nkab txais cov txheej txheem ua tiav ntawm "hluav taws xob arc rauv smelting, LF refining, VD nqus degassing, kub dov, tho, txias txias / txias dov kub kho". Raws li cov ntaub ntawv tsim khoom los ntawm cov neeg muag khoom hauv tsev, cov ntsiab lus tseem ceeb ntawm kev tswj xyuas zoo suav nrog:

1. Pure steel smelting: Sulfur (S) thiab phosphorus (P) cov ntsiab lus yuav tsum muaj tsawg dua los yog sib npaug li 0.010%, thiab tsis yog -hlau inclusions yuav tsum tau tswj hauv qib 1.5;

2. Kev tswj kev ua haujlwm kub: Kev ntsuas qhov ntsuas kub yuav tsum tau tswj hwm ntawm 1150 ± 20℃kom tsis txhob muaj qhov tsim ntawm δ-ferrite;

3. Cov txheej txheem kev kho cua sov: Kev kho dual ntawm "normalizing (1050℃× 30min) + tempering (760℃× 60min)" yog siv los xyuas kom meej lub microstructure yog tempered martensite;

4. Tsis yog- kuaj kev puas tsuaj: 100% eddy kev kuaj tam sim no + kuaj ultrasonic, nrog kev kuaj pom qhov tsis xws luag ncav cuag Φ0.5mm tiaj- hauv qab qhov.

Qhov tseem ceeb, tus neeg muag khoom siv "peb- yob nruam dov zeb + online quenching" thev naus laus zis, ua rau cov khoom lag luam tawm los rau 92%, kev txhim kho 15% piv rau cov txheej txheem ib txwm muaj.

 

A213 T92 Boiler raj siv

1. Kev lag luam fais fab:

- High-kub reheater raj bundles rau ultra-supercritical units (600℃/ 620 degree), ua haujlwm ntawm qhov kub txog li 610℃;

- Cov ntaub ntawv tshaj tawm los ntawm 1,000 MW chav tsev qhov project qhia tau hais tias siv T92 steel tubes nce boiler thermal efficiency mus rau 45.5% thiab txo cov thee noj los ntawm 12 g / kWh.

2. Petrochemical Kev Lag Luam:

- Hydrogenation reactor pipelines, resistant rau hydrogen ib puag ncig ntawm 540℃thiab 20 MPa;

- Cov ntaub ntawv tshawb fawb los ntawm kev ua kom zoo thiab tshuaj ua lag luam qhia tias T92 cov kav dej muaj lub neej ua haujlwm txog li 15 xyoo, 60% ntev dua li cov khoom siv niaj hnub.

3. Nuclear fais fab kev lag luam:

- Cov raj xa hluav taws xob rau cov tshuab hluav taws xob hauv plaub - tiam siab - cov pa kub kub - cov reactors txias, ua rau muaj kev tiv thaiv zoo rau cov hluav taws xob neutron o.

 

SA213 T92 Alloy steel yeeb nkab Hoobkas