A312 TSO 304
Sep 13, 2023
Product Description
A312 yeeb nkab yog tsim raws li ASTM (American Society for Testing and Materials) cov qauv. ASTM A312 tshwj xeeb yog tsim los rau seamless thiab welded austenitic stainless hlau yeeb nkab rau kub kub thiab dav siv corrosion. "TP304" yog hais txog hom 304 stainless hlau, uas yog ib hom thiab dav siv stainless hlau alloy. Hom 304 yog ntau yam thiab nrov austenitic stainless hlau alloy uas muaj kev sib xyaw ntawm chromium thiab npib tsib xee. Nws muaj kev tiv thaiv zoo corrosion thiab zoo formability thiab yog feem ntau siv nyob rau hauv ntau yam kev siv xws li piping, industrial khoom, khoom noj khoom haus, thiab lwm yam.
A312 TP304 Specification
|
Yam khoom
|
A312 TSO 304 | |
|
Qib hlau
|
200/300/400 series
|
|
|
Txuj |
ASTM A213, A312, ASTM A269, ASTM A778, ASTM A789, DIN 17456, DIN17457, DIN 17459, JIS G3459, JIS G3463, GOST 9941, EN10216, BS3605,
GB13296 |
|
|
Khoom siv
|
304, 304L, 309S, 310S, 316,316Ti, 317,317L, 321,347,347H, 304N, 316L, 316N, 201,
202 |
|
|
Nto
|
Polishing, annealing, pickling, ci
|
|
|
Hom
|
kub dov thiab txias dov
|
|
|
stainless hlau round yeeb nkab / raj
|
||
|
Loj |
Phab ntsa thickness
|
1mm-150mm(SCH10-XXS)
|
|
Sab nraud txoj kab uas hla
|
6mm-2500mm (3/8"-100")
|
|
|
Lub sij hawm xa tuaj
|
Kev xa khoom sai lossis raws li kev txiav txim kom muaj nuj nqis.
|
|
|
Pob
|
Txheem export seaworthy pob, los yog raws li xav tau.
|
|
|
Daim ntawv thov |
Siv dav hauv roj av, khoom noj khoom haus, tshuaj lom neeg kev lag luam, kev tsim kho, hluav taws xob, nuclear, zog, tshuab, biotechnology, ntawv
ua, shipbuilding, boiler teb. Cov kav dej kuj tuaj yeem ua raws li tus neeg yuav tsum tau ua. |
|

Tshuaj muaj pes tsawg leeg
| Qib | C | Mn | P | S | Si | Ni | Cr | Fe |
|---|---|---|---|---|---|---|---|---|
| TIAB SA 304 | 0.08 | 2.00 | 0.045 | 0.030 | 1.0 | 8-11 | 18-20 | Bal. |
Mechanical Properties
| Tensile zog (Mpa) Max | Yield Point (Mpa) Max | Elongation (%) | Hardness (HRB) Max | |
|---|---|---|---|---|
| TIAB SA 304 | 515 | 205 | 35 | 92 |
GNEE Profile
GNEE Steel nyob hauv Henan Xeev nrog kev thauj mus los yooj yim. Peb lub tuam txhab yog lub tuam txhab loj tshwj xeeb hauv kev tsim cov kav dej seamless steel, welded steel kav, stainless hlau kav, galvanized kav thiab lwm yam steel kav. Peb tsuas yog tsim cov kav hlau tsis muaj steel, cov kav dej tiv thaiv corrosion, cov kav hlau alloy, cov kav dej carbon steel, cov kav dej square, cov kav dej galvanized thiab lwm yam ntaub ntawv. Peb cov khoom siv dav siv hauv kev tsim kho, txuas hniav, kev tsim tsheb, kev teeb tsa hluav taws xob, mining thiab lwm yam. Peb tau txais kev lees paub los ntawm peb cov neeg siv khoom nrog peb cov credit thiab kev pabcuam zoo. Nrog nws cov khoom zoo zoo thiab kev pab cuam tom qab muag, lub tuam txhab tau tsim kev sib raug zoo nrog ntau lub tuam txhab txawv teb chaws.