API 5L X52 PSL2 Seamless Steel Yeeb Nkab
Aug 16, 2023
Khoom Description
API 5L X52 PSL2 Seamless Steel Yeeb Nkab yog cov yeeb nkab zoo steel dav siv hauv kev lag luam roj thiab roj. Nws yog tsim los ntawm cov khoom siv zoo tshaj plaws uas ua rau nws muaj zog heev thiab kav ntev. Cov tubing yog tsim los tiv thaiv kev kub ntxhov thiab huab cua kub heev rau siv nyob rau hauv ib puag ncig nyuaj.
|
Khoom npe |
API 5L X52 PSL2 Seamless Steel Yeeb Nkab |
|
Txuj |
ASTM A106, ASTM A53, API 5L Gr.B, DIN17175, DIN1629 |
|
Sab nrauv Dia: |
20mm -610 hli |
|
Phab ntsa Thickness |
4mm -70 hli |
|
Dia Tolerance |
Tswj nrog hauv tus qauv, OD: ntxiv rau -1 feem pua, WT: ntxiv rau -10 feem pua |
|
Khoom siv |
10 #, 20 #, 45 #, 16Mn, A106 (B, C), A53 (A, B), API J55, API K55, Q235, Q345, ST35.8, ST37, ST42, ST45, ST52 |
|
Kev tshuaj xyuas |
ISO, BV, SGS, MTC |
|
Ntim |
Waterproof ntawv, thiab steel sawb ntim. Standard Export Seaworthy Package.Suit rau txhua yam kev thauj mus los, lossis raws li qhov xav tau |
|
Muaj peev xwm muab khoom |
1000 metric tons / hli |
|
MOQ |
5 metric ton, qauv txiav txim txais |
|
Lub sijhawm khoom xa tuaj |
Hauv 7-10 hnub ua haujlwm tom qab tau txais qhov tso nyiaj lossis L/C |
|
Kev them nyiaj |
T / T, LC |
|
Muaj peev xwm |
250, 000 tons / xyoo |

Product Mechanical Performance Table:
| Khoom | Kev xav tau |
|---|---|
| Yield zog | Ntau dua lossis sib npaug rau 52, 000 psi (360 MPa) |
| Tensile zog | Ntau dua lossis sib npaug rau 66, 000 psi (455 MPa) |
| Elongation | Ntau dua lossis sib npaug li 21 feem pua |
Product Element Table:
API 5L X52 PSL2 steel nta tswj qib ntawm cov ntsiab lus tseem ceeb:
| Element | Kev sib xyaw (%) |
|---|---|
| Cov pa roj carbon | 0.16 - 0.45 |
| Manganese | 1.65 max |
| Phosphorus | 0.020 max |
| Sulfur | 0.010 max |
| Silicon | 0.45 max |
| Chromium | 0.50 max |
| Nickel | 0.50 max |
| Molybdenum | 0.15 max |
Cov khoom siv
API 5L X52 PSL2 Seamless Pipe yog dav siv nyob rau hauv ntau yam lag luam:
Roj thiab Roj Kev Lag Luam: Cov kav dej no yog qhov tseem ceeb rau kev nyab xeeb ntawm cov roj av, roj av thiab lwm yam hydrocarbons los ntawm cov kav dej.
Zog infrastructure: X52 PSL2 pipelines ua lub luag haujlwm tseem ceeb hauv kev thauj mus los ntawm hluav taws xob, suav nrog cov kav xa hluav taws xob hla teb chaws thiab kev faib khoom sib txuas.
Petrochemical kev lag luam: siv nyob rau hauv petrochemical nroj tsuag thiab refineries los thauj ntau yam tshuaj thiab gases.