ASTM A333 GR.6 steel yeeb nkab
Oct 13, 2023

A333 Qib 6 Yeeb Nkab Specification
| ASTM A333 GR. 6 Carbon Steel Pipes Cov Qauv | ASTM, ASME thiab API |
| Carbon Steel ASTM A333 Yeeb Nkab Lwm Qib | A333 Qib 1, A333 Qib 3, A333 Qib 4, A333 Qib 6, A333 Qib 7, A333 Qib 8, A333 Qib 9, A333 Qib 10, A333 Qib 11 Seamless Pipes |
| ASTM A333 GR. 6 Carbon Steel Round Pipes Loj | 1/2 "NB to 36" NB |
| Carbon Steel A333 GR.6 Seamless Yeeb Nkab Thickness | 3-12 hli |
| ASTM A333 Qib 6 Pipes Schedules | SCH 40, SCH 80, SCH 160, SCH XS, SCH XXS, Tag nrho cov sij hawm |
| Carbon Steel A333 Qib 6 Yeeb Nkab Keeb Kwm | Teb chaws Europe, Nyiv, Kauslim Teb, Asmeskas, Khab (Tshwj tsis muaj cov khoom siv Suav) |
| ASTM A333 Carbon Steel GR.6 Seamless Pipes kam rau ua |
Cold drawn yeeb nkab: +/- 0.1mm Cov yeeb nkab txias txias: +/- 0.05mm |
| ASTM A333 Gr 6 Carbon Steel Pipe Khoom siv tes ua | Cold rolled thiab Cold drawn |
| Carbon Steel A333 Gr.6 Rectangular Pipe Hom | Seamless / ERW / Welded / Fabricated / CDW |
| ASTM A333 Gr.6 Carbon Steel Welded Pipes Daim Ntawv | Hloov, Hydraulic thiab lwm yam |
| Carbon Steel A333 Gr.6 Square Yeeb Nkab Ntev | Min 3 Meters, Max18 Meters, los yog raws li tus neeg yuav tsum tau muaj |
| ASTM A333 Qib 6 CS Pipes End | Plain End, Beveled kawg, Treaded |
| ASTM A333 GR. 6 Carbon Steel Welded Pipes Tshwj xeeb hauv | Loj Dia ASTM A333 Qib 6 Yeeb Nkab |
| ASTM A333 LSAW Pipes Ntxiv Kev Ntsuas | NACE MR0175, NACE TM0177, NACE TM0284, HIC TEST, SSC TEST, H2 SERVICE, IBR, thiab lwm yam. |
ASTM A333 Qib 6 Carbon Steel Seamless Yeeb Nkab Chemical Composition
| C (max) | Mn | P (max) | S (max) | Si | Ni | |
| Qib 1 | 0.03 | 0.40 – 1.06 | 0.025 | 0.025 | ||
| Qib 3 | 0.19 | 0.31 – 0.64 | 0.025 | 0.025 | 0.18 – 0.37 | 3.18 – 3.82 |
| Qib 6 | 0.3 | 0.29 – 1.06 | 0.025 | 0.025 | 0.10 (min) |
ASTM A333 Qib 6 Carbon Steel Seamless Yeeb Nkab Tawm Thiab Tensile Zog
| ASTM A333 Qib 1 | |
| Yam tsawg kawg nkaus | 30,000 PSI |
| Yam tsawg kawg nkaus Tensile | 55,000 PSI |
| ASTM A333 Qib 3 | |
| Yam tsawg kawg nkaus | 35,000 PSI |
| Yam tsawg kawg nkaus Tensile | 65,000 PSI |
| ASTM A333 Qib 6 | |
| Yam tsawg kawg nkaus | 35,000 PSI |
| Yam tsawg kawg nkaus Tensile | 60,000 PSI |
Lub tuam txhab kom zoo dua
Lub tuam txhab lub zog tseem ceeb suav nrog kev muaj peev xwm ua tau zoo, cov khoom lag luam dav dav, cov txheej txheem ntau lawm, cov saw hlau ruaj khov thiab thev naus laus zis tshiab. Lub tuam txhab muaj peev xwm ua tau raws li kev xav tau ntawm kev ua lag luam, muab cov khoom zoo siab - steel hlau, thiab tuav txoj haujlwm tseem ceeb hauv kev lag luam sib tw.