ASTM A53 Teem caij 80 Pipe
Sep 27, 2023

Qhov ntau thiab tsawg ntawm Carbon Steel ASTM A53 Qib B Welded Yeeb Nkab
| Size NPS | cev OD | Phab ntsa Thickness | Lub cev ID | Nyhav ib ko taw | Standard rau XXHY | Teem caij Cov yeeb nkab # |
Ntu Modulus | Gallon Peev Xwm Ib Kab Tawm |
| 1/2 | 0.84 | 0.109 | 0.622 | 0.85 | STD | 40 | .0407 | .0158 |
| 0.147 | 0.546 | 1.09 | XHY | 80 | .0478 | .0122 | ||
| 0.188 | 0.464 | 1.31 | 160 | .0528 | .0088 | |||
| 0.294 | 0.252 | 1.72 | XXHY | .0577 | .0026 | |||
| 3/4 | 1.05 | 0.113 | 0.824 | 1.13 | STD | 40 | .0705 | .0277 |
| 0.154 | 0.742 | 1.48 | XHY | 80 | .0853 | .0225 | ||
| 0.219 | 0.612 | 1.95 | 160 | .1006 | .0153 | |||
| 0.308 | 0.434 | 2.44 | XXHY | .1103 | .0077 | |||
| 1 | 1.315 | 0.133 | 1.049 | 1.68 | STD | 40 | .1328 | .0449 |
| 0.179 | 0.957 | 2.17 | XHY | 80 | .1606 | .0374 | ||
| 0.250 | 0.815 | 2.85 | 160 | .1904 | .0271 | |||
| 0.358 | 0.599 | 3.66 | XXHY | .2136 | .0146 | |||
| 1 1/4 | 1.66 | 0.140 | 1.380 | 2.27 | STD | 40 | .2346 | .0777 |
ASTM A53 Txuj: ASTM A53 yog cov qauv siv dav dav rau ob leeg seamless thiab welded steel kav. Nws npog ntau qib thiab hom carbon steel kav uas npaj rau kev siv sib txawv.
Qib B: ASTM A53 Qib B yog ib qho ntawm cov qib uas tau teev tseg hauv tus qauv. Nws yog qib ntau dua thiab siv dav, tshwj xeeb tshaj yog nyob rau hauv cov ntawv thov uas muaj qhov kub thiab txias los yog qhov chaw siab.
Yam ntxwv:
ASTM A53 Qib B kav dej feem ntau yog dub lossis kub-dip galvanized.
Lawv siv rau ntau yam kev siv, suav nrog kev xa cov pa roj, dej, roj, thiab lwm yam kua dej.
Cov kav dej no tsim nyog rau kev siv tshuab thiab cov txheej txheem.
Phab ntsa Thickness:
ASTM A53 cov kav dej tuaj yeem sib txawv ntawm phab ntsa thicknesses, nrog rau cov npe xws li Teem sijhawm 40, Teem sijhawm 80, thiab lwm yam. Cov phab ntsa tshwj xeeb tuaj yeem sib txawv raws li daim ntawv thov thiab cov kev xav tau.
Mechanical Properties:
ASTM A53 Qib B cov kav dej muaj cov khoom siv tshwj xeeb, suav nrog lub zog tensile, lub zog tawm los, thiab elongation, raws li tau hais tseg hauv tus qauv. Cov khoom no ua kom cov kav dej muaj peev xwm tiv taus cov khoom hnyav thiab kev ntxhov siab.
Tshuaj muaj pes tsawg leeg:
Cov tshuaj muaj pes tsawg leeg ntawm ASTM A53 Qib B kav kuj tau txhais los ntawm tus qauv, kom ntseeg tau tias cov hlau siv tau raws li qee yam kev cai tshuaj los xyuas kom meej kev ua tau zoo thiab kav ntev.
Kev siv:
ASTM A53 Qib B kav dej yog siv rau ntau yam kev siv, suav nrog cov kav dej, HVAC systems, kev tsim kho, roj thiab roj tsheb thauj mus los, thiab lwm yam.