Kev sib piv ntawm Alloy Steel Thiab High Carbon Steel
Mar 13, 2024
- tsis zoo hardenability ntawm high-carbon steel
Carbon steel xaiv ntawm dej quenching, nws tseem ceeb heev quenching rau hauv txoj kab uas hla ntawm 15 ~ 20mm, rau qhov chaw nrog ib txoj kab uas hla ntau tshaj 20mm, txawm tias cov dej quenching yuav tsis quenched, tsis tuaj yeem xyuas kom meej tias tag nrho cov seem kom tau txais tib yam kev siv tshuab. khoom. Yog li ntawd, rau qhov chaw loj nrog cov kev xav tau siab, carbon steel yeej tsis siv. Thiab hlau alloy steel muaj siab hardenability, yuav siv tau los tsim cov ntoo khaub lig-section loj, complex duab qhov chaw.
- lub siab kub lub zog ntawm high carbon steel yog tsawg, tsis zoo liab hardness
Cov pa roj carbon steel yog siv ntawm qhov kub siab tshaj 200 degree, nws lub zog thiab hardness yuav txo tau sai. Thiab alloy steel tempering stability. Liab hardness yog qhov zoo, tuaj yeem ua haujlwm ntawm qhov kub thiab txias.

- siab carbon steel tsis tuaj yeem tau txais kev ua tau zoo tag nrho
Piv txwv li, kev siv tempering kev kho mob los sim kom tau ib tug zoo tag nrho cov kev ua tau zoo, yog hais tias koj xav kom lub siab zog, lub toughness yog tsawg, yog hais tias koj xav kom zoo toughness, lub zog yog tsawg. Qhov no yog vim tsis zoo tempering stability ntawm carbon steels. Yog li ntawd, cov pa roj carbon steel kom tau txais kev ua tau zoo tag nrho yog qhov phem dua li cov hlau alloy, uas yog, alloy steel muaj qhov zoo ntawm toughness.
- high carbon steel tsis muaj cov khoom tshwj xeeb
Piv txwv li, qhov yuav tsum tau muaj qhov kub-kub hardness los yog nro, oxidation, corrosion kuj, tshwj xeeb hluav taws xob, sib nqus zog, thiab lwm yam., nrog carbon steel tsis tuaj yeem tau, tsuas yog siv cov hlau alloy kom tau raws li cov kev cai saum toj no. Cov pa roj carbon steel kuj muaj qee qhov zoo, xws li los ntawm kev hloov nws cov ntsiab lus carbon thiab kev kho cua sov tsim nyog, koj tuaj yeem tau txais ntau yam kev tsim khoom tsim nyog ntawm kev ua haujlwm. Vim tias tus nqi qis ntawm cov pa roj carbon steel, yooj yim rau kev tsim, kev ua haujlwm zoo, tseem yog cov khoom siv hlau siv dav tshaj plaws hauv kev lag luam, suav txog ntau dua 80 feem pua ntawm tag nrho cov hlau.

Cov saum toj no yog qhov sib txawv ntawm alloy steel thiab siab carbon steel rau koj, yog tias koj xav tau alloy steel yeeb nkab thiab siab carbon steel yeeb nkab thov koj xav tiv tauj peb, peb yuav hais rau koj sai li sai tau.