Qhov sib txawv ntawm A36 thiab A500

Mar 21, 2024

1. A36
ASTM A36 steel yog ib qho ntawm cov kub kub dov hlau.
A36 yog tsim los ntawm ASTM American Society for Testing and Materials.
Nws yog cov pa roj carbon tsawg nrog cov ntsiab lus carbon ntawm {{0}}.25 rau 0.29 ib xees.
Qhov "36" hauv A36 tseem ceeb heev vim nws sawv cev rau qhov tsawg kawg nkaus lub zog tensile ntawm A36 ntawm 36, 000 psi.
A36 yog machinable heev, weldable thiab muaj cov cuab yeej zoo heev.
Qhov no yog ib qho ntawm cov laj thawj rau nws cov koob npe nrov.
Nws kuj yog ib feem ntawm qhov laj thawj yog vim li cas nws thiaj li siv dav hauv cov qauv siv.

A36 Structural Tube
2. A500
ASTM A500 yog lwm yam qis carbon kub dov hlau.
Nws muaj cov tshuaj muaj pes tsawg leeg txog li 0.26 feem pua ​​carbon thiab zoo ib yam li ASTM A36.
Qhov sib txawv tseem ceeb ntawm ASTM A500 thiab ASTM A36 yog cov duab muaj rau txhua hom kub dov hlau.
A36 muaj nyob rau hauv round bar, rectangular bar, square bar, channel, lub kaum sab xis, phaj, round yeeb nkab thiab ncej tshuab, thaum A500 tsuas yog siv rau puag ncig yeeb nkab.
Cov ntawv thov rau ASTM A500 zoo ib yam li lwm cov hlau uas tsis tshua muaj kub dov.
Lawv tau siv ntau heev hauv kev siv cov qauv.

A500 Structural Tube