200 Series D7S
Cov lus piav qhia: Cov ntsiab lus nickel ntawm D7S yog kwv yees li 2.5 feem pua, qis dua me ntsis ntawm D11, thiab tus nqi kuj tseem qis. Stainless hlau nrog 1 feem pua nickel cov ntsiab lus yuav yog cov khoom tseem ceeb hauv D7S kev ua lag luam rau qee qhov, yog li nws tseem yuav yog ib feem tseem ceeb ntawm cov phiaj xwm muag hauv cov cheeb tsam uas muaj kev sib tw siab thiab kev ua tau zoo ntawm kev siv stainless hlau.
Daim ntawv thov teb: Lub hom phiaj kev lag luam rau cov khoom tshiab, xws li stainless hlau chav ua noj thiab cov khoom siv, yog los tsim ib qho kev npaj muag khoom rau cov kav hlau stainless hauv kev ua lag luam.
Bidirectional
Cov lus piav qhia: Lub zog tensile ntawm cov khoom no yog 980-1180MPa, thiab qhov siab tshaj plaws ua haujlwm kub tuaj yeem ncav cuag 90 degree .
Daim ntawv thov teb: Pipeline rau hnyav underwater ib puag ncig
Hom boiler
Cov lus piav qhia: Ultra (ultra) cov chav tseem ceeb yog lub hauv paus rau kev kho tshiab ntawm cov khoom siv hluav taws xob tsim hluav taws xob thiab kev txuag hluav taws xob thiab txo qis emission. Ntawm cov ntsiab lus tseem ceeb ntawm cov boilers supercritical, lub superheater thiab reheater muaj qhov kub thiab txias ua haujlwm siab tshaj plaws thiab qhov chaw ua haujlwm hnyav tshaj plaws. Yav dhau los, tag nrho cov ntaub ntawv siv hauv Suav teb tau raug xa tawm los ntawm txawv teb chaws, thaum tsuas yog 10 hlau thiab hlau cov khoom lag luam hauv ntiaj teb muaj peev xwm tsawg. Cov ntaub ntawv zoo li no nyob rau hauv qhov sib txawv loj, kim kim rau ntshuam, nyuaj rau kev yuav khoom, thiab cov khoom siv luv luv, uas cuam tshuam loj heev rau kev tsim khoom ntawm Tuam Tshoj lub tshuab hluav taws xob ultra Supercritical thiab kev tsim hluav taws xob hluav taws xob. Qhov kev thov tam sim no rau lub tshuab hluav taws xob boiler hauv Suav teb yog kwv yees li 30000 tons hauv ib xyoos, thiab nrog kev txhim kho txuas ntxiv ntawm supercritical (ultra supercritical) lub tshuab hluav taws xob tsim hluav taws xob, qhov kev thov tau nthuav dav txhua xyoo. Ntau lub tuam txhab loj hauv tebchaws tau nqis peev ntau ntawm cov neeg ua haujlwm thiab cov peev txheej nyiaj txiag hauv kev tshawb fawb thiab tsim cov khoom zoo li no, thiab tau ua tiav cov txiaj ntsig tseem ceeb. Ntawm qhov tod tes, nws tau ua nws tus kheej pab rau txoj kev loj hlob ntawm lub teb chaws lub hwj chim kev lag luam, thaum tseem coj nyiaj txiag txiaj ntsim rau lub lag luam.
Daim ntawv thov teb: Hauv kev lag luam fais fab boiler, feem ntau yog nyob rau hauv qhov tseem ceeb xws li superheaters thiab reheater high-temperature seem.