Lub zog ntawm Plain Carbon Steel Pipes

Jul 24, 2023

news-500-500

Lub zog ntawm cov pa roj carbon steel yeeb nkab yog nyob ntawm cov yam ntxwv xws li nws cov qib tshwj xeeb, cov txheej txheem tsim khoom thiab lub xeev kev kho mob. Lub zog ntawm cov pa roj carbon steel yeeb nkab feem ntau yog ntsuas los ntawm kev siv zog, tensile zog thiab elongation. Cov hauv qab no yog lub zog dav dav ntawm cov pa carbon steel yeeb nkab:

Yield zog: Lub zog tawm los ntawm cov pa roj carbon steel yeeb nkab feem ntau yog nruab nrab ntawm 240 MPa thiab 450 MPa, thiab cov qib sib txawv thiab cov ntsiab lus ntawm cov yeeb nkab steel yuav muaj zog sib txawv.

Tensile Strength: Lub zog tensile ntawm cov pa carbon steel yeeb nkab feem ntau yog nruab nrab ntawm 410 MPa thiab 690 MPa, uas tej zaum yuav txawv nrog cov qib sib txawv thiab kev kho mob.

Elongation: Lub elongation ntawm cov pa roj carbon steel yeeb nkab feem ntau yog li ntawm 20 feem pua ​​​​mus rau 30 feem pua, uas yog hais txog lub peev xwm ntawm cov khoom kom deform hauv nro ua ntej tawg.

Nws yog ib qho tseem ceeb uas yuav tsum nco ntsoov tias cov txiaj ntsig no tsuas yog qhov dav dav rau cov pa roj carbon steel yeeb nkab, thiab qhov tseeb lub zog yog nyob ntawm qib tshwj xeeb, cov qauv tsim khoom thiab kev ua cov yeeb nkab. Thaum xaiv cov pa roj carbon steel yeeb nkab, nws yog ib qho tsim nyog yuav tsum xaiv cov qib tsim nyog thiab cov lus qhia tshwj xeeb raws li cov ntawv thov tshwj xeeb kom ntseeg tau tias nws lub zog tuaj yeem ua tau raws li qhov xav tau ntawm qhov project lossis siv. Nyob rau tib lub sijhawm, hauv kev siv tshwj xeeb, tej zaum yuav tsim nyog los xaiv lub zog siab alloy steel yeeb nkab lossis lwm yam khoom tshwj xeeb.