Qhov txawv ntawm A333 GR 3 Thiab GR 6 yog dab tsi
Sep 21, 2023

muaj qee qhov sib txawv ntawm ob qib no:
Yam tsawg kawg nkaus Impact Test Temperature:
A333 Qib 3: Qhov ntsuas qhov ntsuas qhov tsawg kawg nkaus rau Qib 3 yog -150 degree F (-101 degree ).
A333 Qib 6: Qhov ntsuas qhov ntsuas qhov tsawg kawg nkaus rau Qib 6 yog -50 degree F (-45 degree ).
Yam tsawg kawg nkaus Yield Strength:
A333 Qib 3: Qib 3 muaj qhov tsawg kawg nkaus tawm lub zog ntawm 45, 000 psi (310 MPa).
A333 Qib 6: Qib 6 muaj qhov ua tau zoo ntawm 35, 000 psi (240 MPa).
Tshuaj muaj pes tsawg leeg:
Ob qib muaj cov tshuaj lom neeg zoo sib xws nrog qhov sib txawv ntawm cov ntsiab lus carbon. Qib 3 muaj cov ntsiab lus ntawm cov pa roj carbon ntau dua los txhim kho nws cov khoom kub qis.
Lub Hom Phiaj Kub Kub:
A333 Qib 3 feem ntau yog siv rau cov ntawv thov uas qhov kub tsis tshua muaj siab, xws li cov xwm txheej cryogenic, xav tau.
A333 Qib 6 yog siv rau cov ntawv thov uas qhov ntsuas kub qis tshaj qhov kev pabcuam tsis yog qhov hnyav li Qib 3, feem ntau nqes mus rau -50 degree F (-45 degree ).
Daim ntawv thov:
A333 Qib 3 feem ntau yog xaiv rau cov ntawv txias heev uas cov hlau xav tau los tswj nws cov tawv thiab ductility ntawm qhov kub thiab txias, xws li hauv cov roj liquefied natural gas (LNG) cia thiab thauj.
A333 Qib 6 yog siv nyob rau hauv ntau yam ntawm cov kev siv kub-kub, nrog rau cov qauv uas tsis muaj qhov kub thiab txias kev lag luam thiab kev lag luam siv hauv kev lag luam roj thiab roj, kev lag luam petrochemical, thiab kev tsim hluav taws xob.
Hauv cov ntsiab lus, qhov sib txawv tseem ceeb ntawm A333 Qib 3 thiab Qib 6 yog qhov ntsuas qhov ntsuas qhov tsawg kawg nkaus, qhov ua tau zoo, thiab qhov tshwj xeeb ntawm cov kev pabcuam kub qis uas lawv tau tsim. Thaum xaiv cov qib no, nws yog ib qho tseem ceeb uas yuav tau xav txog qhov kev pab cuam kub thiab qhov cuam tshuam uas yuav tsum tau muaj rau daim ntawv thov tshwj xeeb.
tuam txhab kom zoo dua
Lub tuam txhab tshwj xeeb hauv kev muag khoom txhua xyoo ntawm ntau dua 10 lab tons thiab muab kev pabcuam kev cai rau ntau yam khoom. Kev tswj hwm ntawm lub tuam txhab tau koom nrog kev lag luam steel rau ntau tshaj 20 xyoo, thiab pab pawg tswj hwm muaj kev nplua nuj thiab kev sib raug zoo ntawm kev lag luam nrog cov neeg siv khoom thiab cov chaw tsim khoom. Peb ib txwm ua raws li cov qauv kev lag luam hauv qab no: yeej lub lag luam nrog cov khoom zoo; nyiam cov neeg siv khoom nrog cov nqi sib tw; thiab yeej lub koob npe nrov nrog cov kev pabcuam zoo heev.