Dab tsi yog Cov Khoom Siv Ntawm A213

Dec 10, 2024

A213 cov khoom siv feem ntau yog ferritic thiab austenitic alloy steel hlab, feem ntau siv hauv boilers, superheaters thiab tshav kub exchangers. Cov khoom siv tshwj xeeb muaj xws li hauv qab no:

Tshuaj muaj pes tsawg leeg

Txuj

Qib

C

Si

Mn

P,S

Cr

Mo

V

Cu

Ni

ASTM A 213
ASME SA213

T11

0.05-0.15

0.50-1.00

0.30-0.60

Tsawg dua lossis sib npaug rau 0.025

1.00-1.50

0.44-0.65

/

/

/

T12

0.05-0.15

Tsawg dua lossis sib npaug rau 0.50

0.30-0.61

Tsawg dua lossis sib npaug rau 0.025

0.80-1.25

0.44-0.65

/

/

/

T22

0.05-0.15

Tsawg dua lossis sib npaug rau 0.50

0.30-0.60

Tsawg dua lossis sib npaug rau 0.025

1.90-2.60

0.87-1.13

/

/

/

 

Mechanical zog:

Txuj

Qib

Tensile zog (MPa)

Yield zog (MPa)

Elongation (%)

ASTM A 213
ASME SA213

T11

Ntau dua lossis sib npaug rau 415

Ntau dua lossis sib npaug li 170

Ntau tshaj los yog sib npaug rau 30

T12

Ntau dua lossis sib npaug rau 415

Ntau dua lossis sib npaug rau 205

Ntau tshaj los yog sib npaug rau 30

T22

Ntau dua lossis sib npaug rau 415

Ntau dua lossis sib npaug rau 205

Ntau tshaj los yog sib npaug rau 30

 

ASTM A213 steel raj yog siv dav hauv cov hauv qab no:

1. Petrochemical: Hauv kev lag luam petrochemical, ASTM A213 steel yeeb nkab yog dav siv nyob rau hauv high-temperature thiab high-pressure steam piping systems los muab cov cua sov thiab siab. Piv txwv li, nyob rau hauv cov txheej txheem ntawm cov roj tawg thiab tshuaj lom neeg cov tshuaj tiv thaiv, ASTM A213 steel yeeb nkab tuaj yeem tswj tau qhov kub thiab txias siab kom ntseeg tau tias cov khoom siv tau zoo thiab cov khoom zoo.
2. Fais fab tuag: Hauv kev lag luam fais fab, ASTM A213 steel yeeb nkab yog dav siv hauv chav piping tshuab rau chav turbines thiab thermal fais fab nroj tsuag. Nws tuaj yeem tiv taus qhov kub thiab txias kom ntseeg tau tias lub zog tsim hluav taws xob thiab kev nyab xeeb.
3. Kev tsim kho: Hauv kev tsim kho kev lag luam, ASTM A213 steel yeeb nkab yog dav siv hauv cov cua sov thiab cua txias. Kev siv ASTM A213 steel yeeb nkab muab qhov chaw ruaj khov thiab muaj txiaj ntsig zoo thaum ua kom muaj kev nyab xeeb thiab kav ntev ntawm cov kav dej.

 