A106 B Carbon Steel Yeeb Nkab
A106GRB muaj qhov kub thiab txias tsis kam. Nws qhov kev ua haujlwm siab tshaj plaws tuaj yeem ncav cuag 425 degree, yog li nws tau siv dav hauv ntau lub sijhawm uas yuav tsum tau tiv taus qhov kub siab, xws li thermal fais fab, roj refining, tshuaj lom neeg kev lag luam thiab lwm yam lag luam. Tib lub sijhawm, A106GRB kuj muaj lub zog txhua yam thiab hnav tsis kam, thiab tuaj yeem tiv taus cov khoom siv loj.
Gnee Steel (Tianjin) Co., Ltd. yog ib qho ntawm feem txhim khu kev qha manufacturers thiab lwm tus neeg ntawm a106 b carbon steel yeeb nkab nyob rau hauv Tuam Tshoj, kuj txhawb customized kev pab cuam nrog luv nqi. Txais tos rau cov lag luam wholesale luv nqi a106 b carbon steel yeeb nkab rau muag ntawm no los ntawm peb lub hoobkas. Tiv tauj peb rau cov qauv dawb.
A106 B Carbon Steel Pipe Chaw tsim khoom-GNEE
Product Description
A106GRB, tseem hu ua ASTM A106Gr B, yog cov khoom siv carbon steel yeeb nkab qauv tsim nyog rau qhov kub thiab txias ua haujlwm ib puag ncig. Nws cov khoom tseem ceeb yog hlau, carbon, manganese, silicon thiab lwm yam khoom. Cov khoom siv no muaj cov tawv tawv zoo heev thiab kev tiv thaiv corrosion thiab tuaj yeem siv rau hauv cov kav dej thiab cov hlab ntsha hauv cov roj av, cov roj av, tshuaj lom neeg kev lag luam, nkoj tsim, hluav taws xob thiab lwm yam haujlwm.
A106 B Carbon Pipe Specification
|
O.D
|
OD kam rau ua
|
W.T
|
Thickness kam rau ua
|
|
|
21-219 MAS
|
+/-0.03
|
0.6-14MM
|
+/-0.02
|
|
|
Ntev
|
2-12M, raws li cov neeg siv khoom xav tau
|
|||
|
Txuj
|
ISO 9001, 2008, ASTM A53 / BS 1387-1985
|
|||
|
Khoom siv
|
||||
|
Yam khoom
|
Metallurgy, Mineral & Zog
|
|||
|
Cov txheej txheem
|
Seamless
|
|||
|
Ntim
|
Hauv bundles lossis raws li cov neeg siv khoom xav tau
|
|||
|
Kev siv
|
1.rau kev xa khoom tsis tshua muaj siab xws li dej, roj thiab roj
2.Rau kev tsim kho
|
|||
|
Productivity
|
10000 ton / hli
|
|||
|
Kev ua haujlwm
|
Threading, coupling thiab nrog lub hau yas tiv thaiv
|
|||
|
Kev them nyiaj
|
T / T, L / C (30% tso nyiaj)
|
|||
A106 B steel yeeb nkab

Cov khoom siv tshuab ua haujlwm:
| Khoom | Tus nqi |
|---|---|
| Tensile zog | 60, 000 - 70,000 psi (415 - 485 MPa) |
| Yield zog | 35, 000 - 40,000 psi (240 - 275 MPa) |
| Elongation | 30% min |
| Hardness (HB) | 137 HB |
Product Element Cov ntsiab lus:
| Element | Cov ntsiab lus (% los ntawm qhov hnyav) |
|---|---|
| Cov pa roj carbon (C) | 0.30% max |
| Manganese (Mn) | 0.29 - 1.06% |
| Phosphorus (P) | 0.035% max |
| Sulfur (S) | 0.035% max |
| Silicon (Si) | 0.10% min |
A106 Pipe Loj:
| NPS [DN Designator] | Tshaj | Hauv qab | ||
| hauv. | mm | hauv. | mm | |
| 1/8 txog 1-1/2 [6 txog 40], incl | 1/64 (0.015) | 0.4 | 1/64 (0.015) | 0.4 |
| Tshaj 1-1/2 txog 4 [40 txog 100], incl | 1/32 (0.031) | 0.8 | 1/32 (0.031) | 0.8 |
| Tshaj 4 txog 8 [100 txog 200], incl | 1/16 (0.062) | 1.6 | 1/32 (0.031) | 0.8 |
| Tshaj 8 txog 18 [200 txog 450], incl | 3/32 (0.093) | 2.4 | 1/32 (0.031) | 0.8 |
| Tshaj 18 txog 26 [450 txog 650], incl | 1/8 (0.125) | 3.2 | 1/32 (0.031) | 0.8 |
| Tshaj 26 txog 34 [650 txog 859], incl | 5/32 (0.156) | 4.0 | 1/32 (0.031) | 0.8 |
| Tshaj 34 txog 48 [850 txog 1200], incl | 3/16 (0.187) | 4.8 | 1/32 (0.031) | 0.8 |
Cov txheej txheem tsim khoom:
A106 B Carbon Steel Pipe yog tsim los siv cov txheej txheem tsim khoom seamless uas ua kom muaj kev sib haum xeeb thiab kev ntseeg tau. Cov txheej txheem ntau lawm suav nrog:
Kev xaiv cov khoom siv raw: Cov pa roj carbon zoo yog xaiv rau nws lub zog thiab kav ntev.
Cua sov: Thaum tshav kub kub cov ntaub ntawv raw mus rau qhov zoo forging kub.
Perforation: Lub voj voog steel yog perforated los ua ib lub raj hollow.
Rolling: Lub raj yog dov mus rau qhov xav tau loj thiab phab ntsa tuab.
Kev kho cua sov: Cov kav dej yog kho cua sov los txhim kho cov khoom siv kho tshuab.
Kev Ntsuas: Kev kuaj xyuas zoo kom ua raws li cov qauv kev lag luam.
Finishing: Txheej los yog tiav cov kav dej raws li cov neeg siv khoom xav tau.
GNEE Office & Team

GNEE Group yog cov kws tshaj lij steel yeeb nkab chaw tsim khoom thiab xa tawm. GNEE Group tau tsim nyob rau hauv 2008, los ntawm thawj 5 tus neeg mus rau ntau tshaj 120 tus neeg tom qab 15 xyoo ntawm txoj kev loj hlob. Peb txoj kev loj hlob tsis yog tsuas yog kev loj hlob ntawm pab pawg, tab sis kuj yog kev txhawb nqa ntawm kev paub thiab kev txhim kho ntawm cov kab ke. Niaj hnub no peb yog ib lub tuam txhab muaj kev paub txog uas tuaj yeem muab cov kev pabcuam zoo tshaj plaws thiab cov khoom zoo rau koj. Peb muaj kev paub tab hauv kev tsim khoom, kev muag khoom, kev thauj mus los thiab kev pabcuam, thiab yog koj tus khub zoo tshaj plaws.

Cim npe nrov: A106 B carbon steel yeeb nkab, Tuam Tshoj A106 B carbon steel yeeb nkab manufacturers, lwm tus neeg, Hoobkas
Xa kev nug