A 519 1045 Seamless Steel Yeeb Nkab

Standard: A519 1045 yeeb nkab
Loj: 10-324mm
Thickness: 6-350 hli
Ntev: 14000mm max

Gnee Steel (Tianjin) Co., Ltd. yog ib qho ntawm feem txhim khu kev qha manufacturers thiab lwm tus neeg ntawm 519 1045 seamless steel yeeb nkab nyob rau hauv Tuam Tshoj, kuj txhawb customized kev pab cuam nrog luv nqi. Txais tos rau cov lag luam wholesale luv nqi ib 519 1045 seamless steel yeeb nkab rau muag ntawm no los ntawm peb lub hoobkas. Tiv tauj peb rau cov qauv dawb.

 

A 519 1045 SMLS Pipe Description

CovA519specification muaj ob peb qib ntawm carbon alloyed seamless mechanical yeeb nkab specification . 1045 yog ib tug ntawm cov qib.
Cov lus qhia A519 1045 suav nrog seamless kub- dov txhua yam tubing thiab seamless txias- kos cov tshuab raj hauv qhov ntau thiab tsawg mus txog 12 3/4 (323.8) sab nraud txoj kab uas hla.
A 519 1045 cov hlab yog muab nyob rau hauv ib puag ncig, square, duab plaub lossis hauv cov duab uas tus neeg yuav khoom.

GNEE Group, raws li tus kws tshaj lij A519 1045 cov chaw tsim khoom siv tshuab, tuaj yeem tsim A519 1045 seamless carbon steel round kav, A519 1045 seamless carbon steel square tubes, A519 1045 cua sov-kho carbon steel kav, A519 1045 txias- dov seamless kav, thiab lwm yam steel kav. Raws li cov chaw tsim khoom, peb tuaj yeem muab cov nqi zoo dua li lwm tus neeg muag khoom.

Tiv tauj peb rau tus nqi qis tshaj A 519 1045 seamless yeeb nkab.

A 519 1045 Carbon Pipe Specification

Khoom siv 1045
OD 1 hli ~ 50mm
WT 6mm ~ 350 hli
Ntev 12 m max
Cov txheej txheem Cold Draw / Cold Rolled, Kub Rolled, Kub Fininsh
Nto Anti xeb roj
Xaus tiv thaiv Yas Pipe Cap
Ua siab ntev Nws tuaj yeem tswj tau hauv OD / Thickness +/- 0.1mm
Daim ntawv thov Auto Parts, Machinery Parts
Kuaj Kev Ntsuam Xyuas Kev Nyuaj Siab, Flaring Test, Flange Test, Rov Qab Test, Hardness Test, Hydrostatic lossis Nondestructive Electric Test

Tshuaj muaj pes tsawg leeg ntawm A519 1045 Seamless steel yeeb nkab

Qib Steel Chemical Composition Limits (%)
C Mn P Max. S Max. Si Cr Mo
1045 0.43-0.50 0.60-0.90 0.040 0.050 / / /

Mechanical Properties ntawm ASTM A519 / ASME SA 519 1045 Cov yeeb nkab steel

Qib Qib Yam Khoom Lub cev
Qhov xwm txheej Qhov kawg lub zog Yield zog Elongation hauv 2in (%) Rockwell Hardness B-Scale
Ksi Mpa Ksi Mpa
1045 HR 75 517 45 310 15 80
CW 90 621 80 552 5 90
SR 80 552 70 483 8 85
A 65 448 35 241 20 72
N 75 517 48 331 15 80

SA 519 1045Carbon Steel Mechanical Tube

1045 seamless steel pipes1045 Carbon Steel Seamless Tube

GNEE Carbon Steel Pipe Kev Tshuaj Xyuas

Round Hot-Finished Tubing Test

CS Mechanical Tubing Ntim thiab xa khoom

Mechanical Tubes Packaging and Shipping

FAQ

Q 1: Qhov zoo yog dab tsi?
A: Peb zoo siab txais tos thib peb- tog kev tshuaj xyuas xws li TUV. Tag nrho cov khoom xa tuaj yuav raug xa nrog MTC thiab stamped los ntawm TPI.

Q 2: Lub sijhawm khoom xa tuaj ntev npaum li cas?
A: Yog tias cov khoom muaj nyob rau hauv Tshuag, feem ntau nws yuav siv sij hawm 5-10 hnub. Yog tias cov khoom tsis nyob hauv Tshuag, nws yuav siv sijhawm 15-20 hnub. Nws kuj tuaj yeem nyob ntawm qhov ntau.

Q 3: Koj puas muab cov qauv? Dawb los tsis?
A: Yog, peb tuaj yeem muab cov qauv dawb, tab sis tus nqi thauj khoom yuav tsum tau them los ntawm cov neeg siv khoom.

Q 4: Kuv puas tuaj yeem kho cov yeeb nkab steel?
A: Tseeb, peb tuaj yeem tsim raws li koj xav tau. Koj tuaj yeem xa daim duab kos duab CAD.

Q 5: Puas muaj nqi -cov kev pabcuam ntxiv?
A: Hmoov zoo, peb muaj kev paub dhau los hauv kev lag luam no. Peb lub tsev khaws khoom yog nruab nrog cov cuab yeej tsim nyog rau kev pleev xim sab hauv, txheej, yeeb nkab txiav, sib koom vuam, thiab kev tsim kho tshuab raws li kev thov.

Q 6: Cov nqe lus ntawm kev lag luam yog dab tsi?
A: FOB, CFR, CIF, thiab LC tau txais.

Tus nqi qis, Hu rau tam sim no

Cim npe nrov: A519 1045 Seamless Steel Yeeb Nkab, Tuam Tshoj A519 1045 Seamless Steel Pipe manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

(0/10)

clearall