ASTM SA213 Kub Exchanger Tube
GNEE Group tsim thiab xa tawm A213 T1 Hlau Yeeb Nkab, A213 T5 Hlau Yeeb Nkab, T9 Hlau Yeeb Nkab, T11 Hlau Yeeb Nkab, T12 Hlau Yeeb Nkab, T22 Hlau Yeeb Nkab, T91 Hlau Yeeb Nkab, A213 Hlau Yeeb Nkab tuaj yeem siv rau hauv tshav kub thiab fais fab nroj tsuag, roj thiab roj nroj tsuag, aviation thiab lwm yam kev lag luam.
Gnee Steel (Tianjin) Co., Ltd. yog ib qho ntawm feem txhim khu kev qha manufacturers thiab lwm tus neeg ntawm astm sa213 tshav kub exchanger raj nyob rau hauv Tuam Tshoj, kuj txhawb customized kev pab cuam nrog luv nqi. Txais tos rau cov lag luam wholesale luv nqi astm sa213 kub exchanger raj rau muag ntawm no los ntawm peb lub hoobkas. Tiv tauj peb rau cov qauv dawb.
ASTM SA213 Alloy Steel Pipe Description
|
Khoom npe |
ASTM SA213 / A213 Seamless Alloy steel yeeb nkab; Kub Exchanger Tube; Boiler Tube |
|
Sab nraud |
10--300mm, raws li cov neeg siv khoom xav tau |
|
Thickness |
4--100mm, raws li cov neeg siv khoom xav tau |
|
Ntev |
1--12M, raws li cov neeg siv khoom xav tau |
|
Txuj |
ASTM SA213 thiab lwm yam. |
|
Hom |
Hloov |
|
Xaus |
Bevel End / BE / Buttweld, PE / Plain kawg |
|
Kev kho saum npoo |
Liab qab, Dub Painted, Varnish Txheej, galvanized thiab lwm yam. |
|
Kos npe |
Standard Marking, los yog raws li tus neeg yuav tsum tau muaj. Marking Method: Tsis Siv Neeg Txau Cov Xim Dawb. |
|
Khoom siv |
Hlau yeeb nkab |
ASTM A213 Tube tshuaj muaj pes tsawg leeg
|
Qib |
C |
Mn |
P |
S |
Si |
Cr |
Mo |
V |
N |
Ni |
Al |
Nb |
W |
|
T2 |
0.10-0.20 |
0.30-0.61 |
0.025 max |
0.025 max |
0.10-0.30 |
0.50-0.81 |
0.44-0.65 |
||||||
|
T5 |
0.15 max |
0.30-0.60 |
0.025 max |
0.025 max |
0.50 max |
4.00-6.00 |
0.45-0.65 |
||||||
|
T9 |
0.15 max |
0.30-0.60 |
0.025 max |
0.025 max |
0.25-1.00 |
8.0-10.0 |
0.90-1.10 |
||||||
|
T11 |
0.15 max |
0.30-0.60 |
0.025 max |
0.025 max |
0.50-1.00 |
1.00-1.50 |
0.44-0.65 |
||||||
|
T12 |
0.15 max |
0.30-0.60 |
0.025 max |
0.025 max |
0.50-1.00 |
1.00-1.50 |
0.44-0.65 |
||||||
|
T22 |
0.05-0.15 |
0.30-0.60 |
0.025 max |
0.025 max |
0.50 max |
1.90-2.60 |
0.87-1.13 |
||||||
|
T91 |
0.08-0.12 |
0.30-0.60 |
0.020 max |
0.010 max |
0.20-0.50 |
8.00-9.50 |
0.85-1.05 |
0.18-0.25 |
0.03-0.07 |
0.40 max |
0.04 max |
0.06-0.10 |
|
|
T92 |
0.07-0.13 |
0.30-0.60 |
0.020 max |
0.010 max |
0.50 max |
8.50-9.50 |
0.30-0.60 |
.015-0.25 |
0.03-0.07 |
0.40 max |
0.04 max |
0.04-0.09 |
1.50-2.00 |
ASTM SA213 tshav kub exchangers yog tsim rau seamless hlau caij thiab austenitic steel tubes nrog tsawg kawg nkaus phab ntsa thickness rau boilers thiab superheaters raws li zoo raws li austenitic steel hlab rau tshav kub exchangers.Qhov tseem ceeb ntawm steel tubes yog qib: A213T5, T11, A213T12, A213T22 thiab lwm yam.
Khoom specification: OD 21.3 ~ 760mm, tuab phab ntsa: 2.0 ~ 130mm.
Cov txheej txheem ntau lawm: kub dov, txias kos, kub nthuav dav, tus txheej txheem xa khoom: kev kho cua sov.
Daim ntawv thov:
Nyob rau hauv lub zog sector, nws yog feem ntau siv nyob rau hauv chav pipelines ntawm thermal fais fab nroj tsuag thiab pipelines rau kis tau tus mob ntawm roj thiab natural gas.
Hauv kev lag luam tshuaj, rau cov kav dej xa cov xov xwm corrosive thiab siab -kub tshuaj tiv thaiv.
Hauv kev lag luam aerospace, raws li cov kav dej txias thiab cov qauv kev txhawb nqa rau cov khoom siv cav.
Petroleum refining kev lag luam, koom nrog kev kub siab thiab kev kub siab txheej txheem piping.

Hais txog GNEE
GNEE Service

GNEE Group tau tsim cov raj steel rau 16 xyoo, tsim thiab xa tawm raws li ASTM, JIS, BS, EN thiab lwm yam. GNEE Group tseem tuaj yeem muab koj nrog kev ua, kuaj, ntim thiab xa cov kev pab cuam ntawm cov hlau thiab cov kav dej, yog tias koj xav tau, thov hu rau peb tam sim.
GNEE Certification

FAQ
1. Koj puas yog lub Hoobkas lossis tuam txhab lag luam?
Peb yog lub Hoobkas ua haujlwm tag nrho, thiab peb tau tsim kev sib koom tes nrog cov koom haum koom tes los nthuav peb cov khoom lag luam hauv kev lag luam steel.
2. Kuv tuaj yeem tau txais cov lus hais los ntawm koj li cas?
Xav tias dawb tso peb cov lus, thiab peb cog lus tias yuav teb raws sijhawm rau txhua qhov kev nug.
Tsis tas li ntawd, peb cov ntaub ntawv tiv tauj tau npaj muaj nyob rau ntawm peb nplooj ntawv tiv toj rau koj qhov yooj yim.
3. Kuv puas tuaj yeem tau txais cov qauv ua ntej xaj?
kiag li! Peb muab cov qauv pub dawb thiab tsim los tsim raws li koj cov qauv lossis cov duab kos duab.
4. Koj lub sijhawm xa khoom yog dab tsi?
Kev xa khoom feem ntau yuav siv sijhawm li 10 hnub, ua kom tiav nrawm ntawm koj qhov kev txiav txim.
Rau cov khoom hauv Tshuag, peb lav xa tuaj tsis pub dhau 2 hnub.
5. Koj cov nqe lus them nqi yog dab tsi?
Peb ua haujlwm nrog lub sijhawm them tus qauv ntawm 30% tso nyiaj, haum rau EXW, FOB, CFR, thiab CIF cov nqe lus.
Cim npe nrov: Tuam Tshoj astm sa213 tshav kub exchanger tube manufacturers, lwm tus neeg, Hoobkas