SA213 T22 Alloy Steel Seamless Yeeb Nkab
Lub sij hawm xa tuaj: 15-21 Hnub
Ntev: 1-12m
MOQ: 3 Tons
Gnee Steel (Tianjin) Co., Ltd. yog ib qho ntawm feem txhim khu kev qha manufacturers thiab lwm tus neeg ntawm sa213 t22 alloy steel seamless yeeb nkab nyob rau hauv Tuam Tshoj, kuj txhawb customized kev pab cuam nrog luv nqi. Txais tos rau cov lag luam wholesale luv nqi sa213 t22 alloy steel seamless yeeb nkab rau muag ntawm no los ntawm peb lub hoobkas. Tiv tauj peb rau cov qauv dawb.
SA213 T22 Seamless Alloy Steel Yeeb Nkab Specification
SA213 T22 Seamless Alloy Steel Boiler Pipe Specification
|
Khoom npe |
Seamless Carbon Steel Yeeb Nkab Rau Tsev Khoom |
|
Khoom siv |
T22, T91, P92, thiab lwm yam. |
|
Phab ntsa Thickness |
4.5MM ~ 60MM |
|
Sab nraud |
21.3MM ~ 762MM |
|
Ntev |
Length: Ib qho random ntev / Ob chav random ntev |
|
Tshooj Duab |
Square, Rectangular, Hloov, |
|
Cov txheej txheem |
Seamless Steel Yeeb Nkab |
|
Ntim |
Ntim, lossis nrog txhua yam xim PVC lossis raws li koj xav tau |
|
Cov yeeb nkab kawg |
Plain kawg / Beveled, tiv thaiv los ntawm lub kaus mom yas ntawm ob hnub, txiav quare, grooved, xov thiab coupling, thiab lwm yam. |
|
MOQ |
1 Tons, ntau tus nqi yuav qis dua |
A213 T22 Seamless Yeeb Nkab Tshuaj muaj pes tsawg leeg
| Tshuaj muaj pes tsawg leeg | C | Si | Mn | P | S | Cr | Mo |
|---|---|---|---|---|---|---|---|
| Min | 0.05 | - | 0.3 | - | - | 1.9 | 0.87 |
| Max | 0.15 | 0.5 | 0.6 | 0.025 | 0.025 | 2.6 | 1.13 |
A213 T22 Alloy yeeb nkab Mechanical zog
| Tensile zog σb Mpa |
Yield Point σs Mpa |
Elongation ntawm tawg los yog elongation δ % |
Hardness HBW |
|---|---|---|---|
| Ntau dua lossis sib npaug li 415 | Ntau dua lossis sib npaug rau 205 | Ntau tshaj los yog sib npaug rau 30 | Tsawg dua lossis sib npaug li 163 |
GNEE A213 T22 Seamless Steel Alloy Yeeb Nkab Kev Muag Khoom

ASME SA213 / SA213M T22 alloy seamless yeeb nkab yog ferritic alloy seamless steel yeeb nkab rau boilers, superheaters thiab kub exchangers ntawm American Society of Mechanical Engineers.
Specifications ntawm A213 T22 alloy seamless yeeb nkab: txheej kab 19.05mm ~ 762mm, phab ntsa thickness 2mm ~ 140mm
Cov txheej txheem ntau lawm: kub dov, kos duab txias, kev xa khoom: kev kho cua sov.
Hais txog GNEE
GNEE Service

GNEE Certification

FAQ
Q: Kuv tuaj yeem tau txais ib qho qauv los kuaj xyuas koj qhov zoo? Nws yuav siv sijhawm ntev npaum li cas thiaj tau txais cov qauv?
A: Tom qab tus nqi raug lees paub, peb yuav muab cov qauv dawb rau koj qhov kev ntsuam xyuas.
Tom qab koj paub meej cov ntsiab lus ntawm cov qauv, cov qauv yuav npaj txhij nyob rau hauv 3-7 hnub thiab yuav xa tuaj tsis pub dhau 3-5 hnub los ntawm kev xa khoom sai.
Q: Koj txais txoj kev them nyiaj dab tsi?
A: Peb lees txais T / T, L / C, Western Union, Paypal. 5.
Q: Koj cov nqe lus shipping thiab lub sij hawm xa tuaj yog dab tsi?
A: FOB, CFR, CIF, 15-60 hnub.
Q: Koj puas muaj luv nqi?
A: Peb yuav ua qhov zoo tshaj plaws los pab koj kom tau txais cov luv nqi nrog tus nqi zoo tshaj plaws thiab kev pabcuam zoo tshaj plaws.
Cim npe nrov: SA213 t22 alloy steel seamless yeeb nkab, Tuam Tshoj sa213 t22 alloy steel seamless yeeb nkab manufacturers, lwm tus neeg, Hoobkas
Xa kev nug