ASTM A312 TP 321 Stainless Hlau Seamless Yeeb Nkab

ASTM A312 Tp321 stainless hlau qib kuj hu ua UNS S32100 yog titanium stabilized alloy. 321 stainless hlau yeeb nkab muaj zoo toughness txawm nyob rau hauv qis kub.

 

ASTM A312 TP 321 SS Seamless yeeb nkab

ASTM A312 TP 321 Stainless Hlau Seamless Tube Nqe lus piav qhia

Stainless hlau 321 qib yog austenitic steel khoom qib. Stainless Hlau 321 Cov Yeeb Nkab yog tsim los nrog cov tshuaj zoo tshaj plaws uas muaj chromium thiab npib tsib xee thaum ruaj khov los ntawm titanium. Cov kav dej no muaj lub zog zoo tshaj plaws thiab tuaj yeem siv rau hauv ntau yam ntawm corrosive thiab txo cov xov xwm. 321 stainless hlau kav yuav siv tau ntawm 538 thiab 870 degrees Celsius. Lawv muaj lub zog tensile yam tsawg kawg nkaus ntawm 515mpa thiab qhov tsawg kawg nkaus tawm lub zog ntawm 205mpa. SS 321 qib kav tau yooj yim elongate mus txog 40% thiab muaj ib tug hardness txog li Rockwell 95 HRB.

ASTM A312 TP 321 Stainless hlau yeeb nkab Specification

Khoom npe
ASTM A312 TP321 Stainless Hlau Seamless Yeeb Nkab
Txuj
ASTM AISI JIS DIN BS GB EN
Qib
201, 202, 301, 302, 304, 304L, 310S, 316, 316L, 321, 430, 430A, 309S, 2205, 2507, 2520, 430 , 410, 440, 904Lect, Los yog Customized
Thickness
0 4-50 mm
Ntev
1-12 m
Sab nraud txoj kab uas hla (OD)
10-2000 hli
Ua siab ntev
a) Txoj kab uas hla: +/-0.2mm
b) Thickness: +/{1}}.02mm
c) Ntev: +/-5mm
Daim ntawv pov thawj
ISO, SGS
Nto
Polishing, annealing, daim iav, ci, pickling
Cov duab:
round, square, rectangular, irregular
Daim ntawv thov
kev kho mob, roj av, aerospace, khoom siv kho mob, cua txias, tshuaj lom neeg kev lag luam, electronics, accessories, khoom noj khoom haus, machinery, fais fab tuag, kws
Ntim
hauv pob khoom nrog cov khoom siv dej tsis zoo, rooj ntoo ntoo

Tshuaj muaj pes tsawg leeg ntawm ASTM A312 Tp 321 Stainless Hlau Exhaust Pipe

Qib C Mn Si P S Cr Mo Ni N Lwm yam

321

min.
max


0.08

2.00

0.75

0.045

0.030

17.0
19.0

9.0
12.0

0.10

Ti=5(C+N)
0.70

321H

min.
max

0.04
0.10

2.00

0.75

0.045

0.030

17.0
19.0

9.0
12.0

Ti=4(C+N)
0.70

Mechanical Properties Ntawm ASTM A312 TP 321 seamless ss yeeb nkab

Qib

Tensile zog (MPa) min

Yield Strength 0.2% Pov thawj (MPa) min

Elongation (% hauv 50mm) min

Hardness

Rockwell B (HR B) max

Brinell (HB) max

321

515

205

40

95

217

321H

515

205

40

95

217

Lub cev muaj zog ntawm ASTM A312 TP 321 SS Yeeb Nkab

Qib

Qhov ceev (kg / m3)

Elastic Modulus (GPa)

Mean Coefficient ntawm Thermal Expansion (m/m/0C)

Thermal conductivity (W / mK)

0-1000C

0-3150C

0-5380C

ntawm 1000C

ntawm 5000C

321

8027

193

16.6

17.2

18.6

16.1

22.2

Qib Specifications Rau 321 Stainless Hlau Yeeb & Tubes

Qib

UNS No

Laus British

Euronorm

Swedish SS

Japanese JIS

BS

En

Tsis muaj

Lub npe

321

S32100

321S31

58B, 58C

1.4541

X6CrNiTi18-10

2337

TIAB SA 321

321H

S32109

321S51

1.4878

X10CrNiTi18-10

SUS 321 H

ASTM A312 TP321 Seamless Yeeb Nkab

TP 321 Stainless Steel Seamless Pipes

Tuam txhab Profile

GNEE Steel Pipe yog cov chaw tsim khoom tshwj xeeb hauv kev tshawb fawb, kev tsim kho, kev tsim khoom, kev muag khoom thiab kev pabcuam ntawm stainless hlau yeeb nkab thiab raj, carbon steel yeeb nkab thiab raj, alloy steel yeeb nkab thiab raj thiab lwm yam. Peb nyob hauv Anyang, Henan Xeev nrog kev thauj mus los yooj yim. GNEE tau koom nrog hauv kev lag luam steel yeeb nkab rau ntau tshaj 15 xyoo thiab muaj kev paub ntau lawm. Peb yog ib lub tuam txhab ua ke kev tsim khoom thiab kev ua haujlwm. Lub lag luam tseem ceeb ntawm peb lub tuam txhab: Indonesia, Singapore, Nyab Laj, Malaysia, Philippines, Chile, Mexico, Israel, Spain thiab lwm yam.

stainless steel tubing suppliers

GNEE Cutsomers

stainless round tube customers

Stainless hlau Round Tube Tshuaj xyuas

stainless exhaust tubing inspection

stainless hlau dej yeeb nkab Ntim thiab xa khoom

smls pipe ship

GNEE Exhibition Photos

sanitary tubing Exhibition

Cim npe nrov: astm a312 tp 321 stainless hlau seamless yeeb nkab, Tuam Tshoj astm a312 tp 321 stainless hlau seamless yeeb nkab manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

(0/10)

clearall