ASTM A210 Qib A1 Boiler Pipes Chaw tsim tshuaj paus

Oct 20, 2023

Cov khoom muaj pes tsawg leeg ntawm A210 Qib A1 Boiler Pipes yog dab tsi?
A210 Qib A1 Boiler Pipesyog carbon steel thiab muaj carbon, manganese, phosphorus, sulfur & silicon. Cov khoom muaj pes tsawg leeg tuaj yeem sib txawv nyob ntawm cov txheej txheem tsim khoom thiab cov kev cai tshwj xeeb Tseem, A210 Qib A1 Boiler Pipes feem ntau muaj cov ntsiab lus siab tshaj plaws ntawm 0.27%, qhov siab tshaj plaws manganese cov ntsiab lus ntawm {{ 6}}.93%, thiab cov ntsiab lus sulfur siab tshaj plaws ntawm 0.025%.

GR.A1 A210 Thaum tshav kub kub Exchanger Tubes Chemical Composition:

Qib

C (Max)

Mn

Si (Min)

P (Max)

S (Max)

A1

0.27

Max 0.93

0.10

0.035

0.035

ASME SA210 Standard Pipes Mechanical Properties:

Qib

Tensile zog (Mpa)

Yield zog (Mpa)

Elongation (%)

A1

Ntau dua lossis sib npaug rau 415

Ntau dua lossis sib npaug li 255

Ntau tshaj los yog sib npaug rau 30

ASME SA / ASTM A210 Cold-Finished Tubes Phab Ntsa Thickness kam rau ua

OD hauv. (mm)

Phab ntsa thickness kam rau ua%
Tshaj (+) Hauv qab (-)
1 ½ (38.1) thiab qis dua 20 0
Tshaj 1½ (38.1) 22 0

info-750-750

Lub tuam txhab kom zoo dua

Peb tuaj yeem ua rau feem ntau arades thiab specifications.meet koj qhov kev xav tau sib txawv.peb muaj kev pabcuam zoo thiab txaus siab tom qab muag. ifclients muaj teeb meem. Peb yuav soive nws nyob rau hauv lub sij hawmWe ntim cov khoom yam xyuam xim thiab xa nyob rau hauv lub sij hawm thiab muaj super kev koom tes nrog logistics, yuav pab tau koj txo koj cov nqi yuav khoom.