ASTM A213 T11 Alloy Steel Seamless Tube
Dec 05, 2025
ASTM A213 T11 Seamless alloy tubes piav qhia
T11 Alloy Tubesyog cov tshwj xeeb siab -alloy steel kav cais raws limartensitic tshav kub-resistant steel, feem ntau yog siv nyob rau hauv siab - qhov kub thiab txias ib puag ncig xws li cov cua kub exchangers thiab boiler piping.
Tshuaj muaj pes tsawg leegmuaj xws li carbon (C), silicon (Si), manganese (Mn), phosphorus (P), sulfur (S), thiab alloying ntsiab xws li chromium (Cr), molybdenum (Mo), thiab vanadium (V). Cov ntsiab lus siab Cr/Mo txhim kho corrosion kuj, siab - kub stability, thiab txhua yam khoom, thaum V txhim kho toughness.
Mechanical Properties:
Siab zog / hardness nrog zoo toughness
Tshaj tawm -cov nqi kho cua sov:
Tensile zog:Ntau dua lossis sib npaug li 450 MPa
-Yield zog:Ntau dua lossis sib npaug li 300 MPa
-Hardness:Ntau dua lossis sib npaug li 200 HB
Zoo heev qaug zog thiab corrosion kuj
Kev kho cua sov:
Quenching: ~ 900℃(tuav 2h) → cua txias
Tempering: ~ 650℃(tuav 2h) → cua txias
Qhov tshwm sim microstructure:Tempered martensitexa balanced mechanical zog.
ASTM A213 T11 Tshuaj muaj pes tsawg leeg:
| Chemical Components (%) | |||||||
| Qib | C | Mn | P | S | Si | Cr | Mo |
| T11 | 0.05-0.15 | 0.30-0.60 | Tsawg dua lossis sib npaug li 0.025 | Tsawg dua lossis sib npaug li 0.035 | 0.50-1.00 | 1.00-1.50 | 0.44-0.65 |
Kev kho cua sov yuav tsum tau
| Qib | UNS Number | Thaum tshav kub kub kho hom | Subcritical Annealing los yog Tempering Kub, Min los yog range℃F [degree] |
| T11 | K11597 | tag nrho los yog isothermal anneal normalize thiab temper | 1200 [650] |
ASTM A213 T11 Seamless Alloy Tubes Tensile Requirements thiab Hardness:
| Mechanical Properties | ||||
| Qib | Tensile | Yield | Elongation | Hardness |
| Lub zog (Mpa) | Lub zog (Mpa) | (%) | (HRB) | |
| T11 | Ntau dua lossis sib npaug rau 415 | Ntau tshaj los yog sib npaug rau 220 | Ntau tshaj los yog sib npaug rau 30 | Tsawg dua los yog sib npaug li 85 |
Mechanical Test & Grain Size Requirements
Tensile Test
Rau ntau ntautsawg dua 50 lub cev: Ib qho kev sim los ntawm ib qho qauv.
Rau ntau ntau50 cev: Ib qho kev sim txhua los ntawm cov qauv ntawm ob lub raj.
Flattening Test
Ib qho kev xeem ntawmtxhua qhov kawgntawm ib lub raj tiav rau ib qho,lwm yam tsis yog lub raj siv rau kev sim flaring.
Flaring Test
Ib qho kev xeem ntawmtxhua qhov kawgntawm ib lub raj tiav rau ib qho,lwm yam uas tsis yog lub raj siv rau kev sim flattening.
Hardness Test
Brinell los yog Rockwell hardness testntawm cov qauv ntawm ob lub raj rau ib qho.
Loj Loj
Kev txiav txim loj ntawm cov nplej yuav tsum tau ua rau ntawmib kawg ntawm ib lub raj tiavib tug ntau los xyuas kom meej raws li cov kev cai.