ASTM A213 T9 Alloy Steel Seamless Tube

Nov 05, 2025

A213 T9 Cov Yeeb Nkab A213 yog qhov tshwj xeeb yog tsim los ntawm Asmeskas cov neeg siv khoom siv tshuab (ASME) rau cov neeg siv roj caryoy Nrog lub ratio piv sib xyaw ntawm 9% chromium {{}}}}} Cov khoom siv nyob ruaj khov xws li ultra {8} bolritical fais fab nroj tsuag thiab marine boilers.

 

‌Peb Cov Qauv Tseem Ceeb:‌

‌Siab Kuj:Withstands qhov siab tshaj plaws ua haujlwm siab ntawm 17.5 MPa (ultra-} songcritical boiler txheem).

‌High - kub kuj:Ntev - tsis muaj kev pab kub tsawg dua lossis sib npaug nrog 593 degree, luv}}}} {degree tsis muaj deformation.

‌Qoob qaug zog:Tsis muaj cov kab nrib pleb

‌

Cov Ntawv Thov:‌

‌Fais fab nroj tsuag Boilers:SuperHeater thiab Reheater rau Ultra - Cov Chav Nyob Supercritical (piv txwv li, 600mw thermal fais fab nroj tsuag).

‌Marine Hwj Chim:Siab - h siab boilers rau long Carrier, cov chav dej rau dej hiav txwv- mus rau ntawm DNV ntawv pov thawj).

‌Petrochemical Cov Khoom Siv:Piping rau hydrogenation reactors, siab - kub crade tawg rauv tub (nrog H2s corrosion ristoration).

 

Kev qhia tshwj xeeb

Qhov loj me (seamless)

6.35mm Od rau 101.60mm Od

Tus qauv

ASTM A213, ASME SA213

Cov Qauv Sib Tw

En 10216-2, ASTM A335, GUS 550-75, S50400, WN 1.7386

Khoom

T9, S50400

Khoom siv sib npaug

P9

Ntaus

Tsis ntse

Tshwj Xeeb Hauv

Qhov loj loj uas loj

Phab Ntsa Thickness

Teem sijhawm 3mm txog 15 hli.

Qho ntev

Max 1 ~ 12m

Teem caij

STD, Sch40, Sch80

Puab

Puag ncig, square, duab plaub, hydraulic thiab lwm yam.

Qho ntev

Ib leeg random, ob npaug random & txiav ntev.

Tubing kawg

Dawb kawg, beveled kawg, tsuj las.

 

Tshuaj lom neeg cov tshuaj lom neeg ASTM A213 / ASME SA213 T5 Alloy Steel Smls Leeg:

C, %

Mn,%

P, %

S, %

Si,%

CR,%

Mo,%

0.15 Max

0.30-0.60

0.025 max

0.025 max

0.25-1.00

8.0-10.0

0.90-1.10

Cov Cuab Yeej Siv Cov Neeg Kho Tshuab Astm A213 / ASME SA213 T5 Alloy Steel Smls Leeg:

Lub zog tensile, mpa

Paib lub zog, mpa

Elongation,%

Hardness, Hb

415 Min

205 min

30 Min

179 Max

Sab Nraud Txoj Kab & Kev Ua Phem:

Kub Rolled

Sab nraud lub cheeb, hli

Kev kam, mm

Od tsawg dua los yog sib npaug rau 101.6

+0.4/-0.8

101.6

+0.4/-1.2

190.5

+0.4/-1.6

Txias Drawn

Sab nraud lub cheeb, hli

Kev kam, mm

Od <25.4

±0.10

25.4 tsawg dua los yog sib npaug rau od tsawg dua lossis sib npaug ntawm 38.1

±0.15

38.1

±0.20

50.8 tsawg dua lossis sib npaug nrog OD <63.5

±0.25

63,5 tsawg dua lossis sib npaug nrog OD <76.2

±0.30

76.2 tsawg dua lossis sib npaug ntawm od tsawg dua lossis sib npaug rau 101.6

±0.38

101.6

+0.38/-0.64

190.5

+0.38/-1.14

Phab Ntsa Thickness & Divilance:

Kub Rolled

Sab nraud lub cheeb, hli

Kev zam txim,%

Od tsawg dua los yog sib npaug rau 101.6, wt tsawg dua lossis sib npaug rau 2.4

+40/-0

Od tsawg dua li lossis sib npaug rau 101.6, 2.4

+35/-0

Od tsawg dua li lossis sib npaug rau 101.6, 3.8

+33/-0

OD≤101.6, WT>4.6

+28/-0

OD>101.6, 2.4

+35/-0

OD>101.6, 3.8

+33/-0

OD>101.6, WT>4.6

+28/-0

Txias Drawn

Sab nraud lub cheeb, hli

Kev zam txim,%

Od tsawg dua los yog sib npaug rau 38.1

+20/-0

OD>38.1

+22/-0

 