ASTM A355 P5 Alloy Seamless Steel Yeeb Nkab
Apr 13, 2024
Khoom Description
Seamless yeeb nkab los ntawm kub dov los yog txias kos
Loj: 1/2 "- 24"
Phab ntsa thickness: SCH 40, SCH STD, SCH 80, SCH XS, SCH 160
Ntev: 6 meters, 12 meters lossis customized.
Xaus: PE (Plain End), BE (Beveled Ends)
| Txuj | Qib | Chemical Composition (%) | Mechanical Properties | ||||||||
| C | Mn | P | S | Si | Cr | Mo | Tensil zog Mpa min |
Yield zog Mpa min |
Elongation % min |
||
| A335 | P5 | 0.15 max | 0.30–0.60 | 0.025 max | 0.025 max | 0.50 max | 4.00–6.00 | 0.45–0.65 | 415 | 205 | 30 |
| P9 | 0.15 max | 0.30–0.60 | 0.025 max | 0.025 max | 0.25–1.00 | 8.00–10.00 | 0.90–1.10 | 415 | 205 | 30 | |
| P11 | 0.05–0.15 | 0.30–0.60 | 0.025 max | 0.025 max | 0.50–1.00 | 1.00–1.50 | 0.44–0.65 | 415 | 205 | 30 | |
| P12 | 0.05–0.15 | 0.30–0.61 | 0.025 max | 0.025 max | 0.50 max | 0.80–1.25 | 0.44–0.65 | 415 | 220 | 30 | |
| P22 | 0.05–0.15 | 0.30–0.60 | 0.025 max | 0.025 max | 0.50 max | 1.90–2.60 | 0.87–1.13 | 415 | 205 | 30 | |
Kub Rolled Seamless Steel Yeeb Nkab


Cov khoom kuaj muaj los ntawm GNEE
Tensile xeem: transverse thiab longitudinal
Flattening xeem
Kev kuaj Hardness
Khoov xeem