Dab tsi yog steel yeeb nkab weld X-ray kuaj
Oct 11, 2024
Tam sim no, lub tshuab hluav taws xob soj ntsuam ntawm cov yeeb nkab steel hlau tuaj yeem muab faib ua: X-ray film imaging thiab digital imaging.
X-ray soj ntsuam cov khoom yuav tsum tau
Hlau yeeb nkab weld radiographic tshuaj xyuas yog tias X-rays ncaj qha nkag mus rau cov khoom siv vuam thiab tsim cov duab tsim nyog ntawm cov duab hluav taws xob soj ntsuam los yog cov duab digital. Qhov dub ntawm cov duab hluav taws xob yuav tsum tsis pub tsawg dua 2.0 (qhov dub ntawm qhov vuam yuav tsum tsis pub tsawg dua 1.5); X-rays siv cov duab zoo ntsuas tau teev tseg los ntawm ISO, thiab cov duab zoo ntsuas tau raug xaiv kom sib haum mus rau qhov tob tob. Lub rhiab heev ntawm X-ray zaj duab xis yog zoo dua 2%, thiab dynamic rhiab heev ntawm industrial TV yog zoo dua 4%.

X-ray soj ntsuam technology yuav tsum tau:
(1) Chav tshuaj xyuas zaj duab xis yuav tsum huv, nyob ntsiag to, thiab qhov kub thiab txias. Lub teeb yuav tsum tsaus thiab mos.
(2) Kev soj ntsuam ib puag ncig yuav tsum muaj qhov kub thiab txias.
(3) Txhawm rau kom ntseeg tau tias cov yeeb yaj kiab zoo, qhov zoo ntawm kev txhim kho thiab txhim kho kev ua haujlwm nrog rau lub sijhawm zoo thiab siv tau ntawm cov yeeb yaj kiab yuav tsum tau lees paub nruj me ntsis raws li qhov yuav tsum tau ua.
(4) Kev nyab xeeb irradiation ntawm chav tsaus ntuj yuav tsum tau txiav txim tsis tu ncua. Daim ntawv thov kev kuaj X-ray X-ray kuaj ntawm cov yeeb nkab steel welds feem ntau yog tsom rau qhov ntim qhov tsis xws luag tsim nyob rau hauv cov txheej txheem steel yeeb nkab, xws li tsis muaj fusion, hlaws, pores, tawg, tsis tiav kev nkag, tungsten inclusions thiab lwm yam tsis xws luag.