Dab tsi yog cov muaj pes tsawg leeg ntawm 213 T2

Feb 24, 2025

Dab tsi yog qhov muaj pes tsawg leeg ntawm 213 T2?

 

A213 T2 yog cov khoom siv steel tshwj xeeb siv feem ntau hauv kev tsim cov boiler thiab cov khoom qub.

 

A213 T2 Cov Khoom Siv Tshuaj

muaj pes tsawg C Si Mn P S ① Cr Mo
Lub min 0.1 0.1 0.3 - - 0.5 0.44
Tus zuag 0.2 0.3 0.61 0.025 0.025 0.81 0.65

① Thaum xaj cov ntsiab lus Sulfur ntau dua, qib kawm yog T2S nrog cov lus faj sulfur siab kawg ntawm {}}. 045%.

 

Cov cuab yeej ua haujlwm ntawm A213 T2 yog dab tsi?

 

A213 T2 Cov Khoom Siv Neeg Kho Tshuab

Lub zog tensile
σb
MPa
Paib
σs
MPa
Elongation thaum tawg lossis elongation
δ
%
Kev nyuaj
HBW
Ntau dua los yog sib npaug rau 415 Ntau dua los yog sib npaug rau 205 Ntau dua los yog sib npaug rau 30 Tsawg dua los yog sib npaug rau 163

 

A213 T2 Bolier tubes with high-temperature