API 5L X42 & X52 Pipe Supplier-GNEE

API 5L X42 kab yeeb nkab thiab API 5L X52 kab yeeb nkab (seamless thiab welded) muaj nyob rau hauv ob yam khoom specifications, PSL1 thiab PSL2, rau txhua qib, uas txawv nyob rau hauv cov nqe lus ntawm tshuaj muaj pes tsawg leeg, manufacturing txheej txheem, mechanical zog, kho cua sov, xeem cov ntaub ntawv , traceability thiab lwm yam. Qhov tseeb, X42, X52, thiab lwm yam qhia txog qhov tsawg kawg nkaus yield zog ntawm cov yeeb nkab steel. X42 qib tubes muaj qhov tsawg kawg nkaus lub zog ntawm 42, 000 ksi thiab X52 qib tubes muaj qhov tsawg kawg nkaus lub zog ntawm 52,000 ksi.

API X42 PIPE

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

API 5L X42 VS API 5L X52 Kab Yeeb Nkab Cov Khoom Siv Tshuaj

Qib

C max

Mn max

P max

S max

Si max

X42

 

PSL1

0.26

1.20

0.030

0.030

/

PSL2

0.22

1.30

0.025

0.015

0.45

X52

PSL1

0.26

1.40

0.030

0.030

/

PSL2

0.22

1.40

0.025

0.015

0.45

 

Mechanical Requirements

Qib

Y. S (ksi) min

T. S (ksi) min

Elongation min

X42

PSL1

60

42

28%

PSL2

60-100

42-72

/

X52

PSL1

66

52

21%

PSL2

66-110

52-77

/