A213 T22 chromium-molybdenum Yeeb
A213 T22 chromium-molybdenum tubing yog qhov kub siab ferritic alloy thiab kev kub siab zoo tshaj plaws lub zog thiab corrosion tsis kam.
A213 T22 CR22 CR-MO QOS LASE LOILOY STEEL QHIA
A213 T22 chromium-molybdenum Yeeb Nkab yog qhov kub siab ferritic alloy steel yeeb nkab ntawm 2.25% chromium thiab 1% molybdenum. Ob lub ntsiab ntawm chromium thiab molybdenum ua A213 T22 steel haum rau nws cov pa hluav taws xob zoo, xws li muaj kev lag luam me me, xws li cov kav dej loj thiab lwm yam khoom siv superheater. Tsis tas li ntawd, cov yeeb nkab steel muaj zoo machinability thiab weldability kom tau raws li txoj hlua khi rau ntau yam kev lag luam.
A213 T22 Chrome Moly Seamless Tubes
|
Lub hom phiaj |
ASTM A213 |
|
Teem nqi |
ASTM A213 T2 T2 T9 T22 T91 T91 T91 T92 Seamless Yeeb Nkab |
|
Ntaus |
Seamless Steel Yeeb Nkab |
|
Kev pab cuam |
Dabtsi yog khoov, vuam, decoiling, xuas nrig ntaus, txiav |
|
Moq |
1 TUJ |
|
Lub thawv |
Hlau Sawb Bundles / Loj |
|
Kawg Kev Kho Mob |
Dawb / beveled |
|
Cov ntsiab lus them nqi |
L / CT / T (30% tso nyiaj) |
|
Tej txuj ci tshiab |
Kub dov lub txias dov txias txias kos |
|
Yam ntim |
Txheem Seaworthy Packing |
|
Kev kuaj xyuas |
Tog Soj Ntsuam |
A213 T22 Kev Siv Tshuaj (%)
| muaj pes tsawg | C | Si | Mn | P | S | Cr | Mo |
|---|---|---|---|---|---|---|---|
| Lub min | 0.05 | - | 0.3 | - | - | 1.9 | 0.87 |
| Tus zuag | 0.15 | 0.5 | 0.6 | 0.025 | 0.025 | 2.6 | 1.13 |
A213 T22 Cov Khoom Siv Neeg Kho Tshuab
| Lub zog tensile σb MPa |
paib σs MPa |
Elongation thaum tawg lossis elongation δ % |
Kev nyuaj HBW |
|---|---|---|---|
| Ntau dua los yog sib npaug rau 415 | Ntau dua los yog sib npaug rau 205 | Ntau dua los yog sib npaug rau 30 | Tsawg dua los yog sib npaug rau 163 |
A213 T22 Seamless Alloy Steel Tube



Cov FAQ
Q: Yuav ua li cas txog MOQ? Yog tias kuv thawj qhov kev txiav txim qty yog me, koj puas yuav txais?
A: Peb xav ua qhov zoo tshaj plaws los txhawb koj qhov kev sim qty, yog li txawm tias txawm tias 1 kg tau ok kev koom tes; Vim tias peb muaj kev ntseeg siab txav mus rau thib ob kev txiav txim nrog koj lub tuam txhab hwm.
Q: Koj cov nqe lus them nqi yog dab tsi?
A: Feem ntau ob lub sijhawm them nyiaj rau cov neeg siv khoom tshiab:
1) 30% T / T li DEPOSIT, 70% tshuav nyiaj li cas rau B / L Luam;
2) 100% irevocable L / C thaum pom; yog tias koj xav tau lwm cov lus, Pls xav tiv tauj peb dhau, peb yuav sim peb qhov zoo tshaj plaws.
Q: Ntev npaum li cas yog koj lub sijhawm khoom plig?
A: Peb cov khoom khaws txhua hnub yog ntau tshaj 8000 tons, yog li rau cov khoom loj, tsuas yog xav tau 5 hnub los ntawm cov khoom lag luam; Yog hais tias qhov tshwj xeeb loj los ntawm kev tsim khoom tshiab, khoom xa 7 hnub.
Q: Yuav ua li cas txog cov qauv? Puas yog nws pub dawb lossis ntxiv?
A: Yog, peb xav muab cov qauv ua ntej xaj; Yog tias cov qauv ntawm cov khoom lag luam, nws yuav pub dawb; Yog tias cov qauv los ntawm cov khoom lag luam tshiab, peb yuav tsub qee tus nqi tsim nyog, tab sis tus nqi no yuav raug txiav tawm los ntawm koj thawj daim ntawv xaj kev txiav txim.
Cim npe nrov: A213 T22 chromium-molybdenum Yeeb Nkab, Tuam Tshoj A213 T22 chromium-molybdenum Cov Yeeb Nkab Cov Ntaub Yeeb Nkab, Chaw muag khoom, Hoobkas
Xa kev nug