40MnB Carbon Steel Seamless Yeeb Nkab
40MnB Carbon Steel Seamless Yeeb Nkab
video
40MnB Carbon Steel Seamless Pipe
40MnB Carbon Steel Seamless Pipe
1/2
<< /span>
>

40MnB Carbon Steel Seamless Yeeb Nkab

MOQ: 1 Tuj
Qib: 20 # 45 # 35 #
Lub sij hawm xa tuaj: 22-30 hnub

 

40MnB Carbon Steel Seamless Yeeb Nkab

40MnB Carbon Steel Seamless Pipe yog cov yeeb nkab zoo tshaj plaws ua los ntawm 40MnB carbon steel, paub txog nws lub zog tshwj xeeb thiab ua haujlwm ntev. Qhov no seamless steel yeeb nkab yog tsim los siv cov cuab yeej siv siab heev los xyuas kom meej qhov zoo ntawm sab hauv thiab sab nrauv. Seamless kev tsim kho yuav tsum tsis muaj vuam, yog li cov tubing muaj zog thiab tsis muaj paug. Vim muaj cov ntsiab lus carbon siab, 40MnB carbon steel seamless yeeb nkab muaj hardness zoo thiab hnav tsis kam.

40MnB Carbon Steel Seamless Yeeb Nkab Qhia

Khoom npe

Khoom siv

Txuj

Loj (mm)

Daim ntawv thov

Tsawg kub tube

16 MnDG
10 MnDG
09dg ua
09mn2 wb
06Ni3MoDG
ASTM A333 Cov khoom lag luam

GB/T 18984-
2003
ASTM A333 Cov khoom lag luam

OD: 8-1240*
WT: 1-200

Thov mus rau - 45 degree ~ 195 degree qis kub siab lub nkoj thiab kub kub exchanger yeeb nkab

High-pressure boiler raj

20G
ASTMA 106B UAS
ASTMA 210A UAS
ST45 8-III

GB 5310-1995
ASTM SA 106
ASTM SA 210
DIN 17175-79

OD: 8-1240*
WT: 1-200

Haum rau kev tsim kev kub siab boiler raj, header, chav yeeb nkab, thiab lwm yam

General qauv
ntawm lub cev

10#,20#,45#,27SiMn
ASTM A53A, B
16 ,q345

GB/T 8162-
2008
GB/T 17396-
1998
ASTM A53

OD: 8-1240*
WT: 1-200

Siv rau cov qauv dav dav, kev txhawb nqa engineering, kev siv tshuab, thiab lwm yam

Roj casing

J55,K55,N80,L80
C90,C95,P110

API SPEC 5CT UAS
ISO 11960

OD: 60-508*
WT:4.24-16.13

Siv rau kev rho tawm cov roj los yog roj hauv cov roj Wells casing, siv rau hauv cov roj thiab cov pa roj zoo sidewall

 

40MnB Carbon Steel Seamless Pipe

Khoom siv industrial:
40MnB carbon steel seamless yeeb nkab yog dav siv nyob rau hauv roj thiab roj, petrochemical, machinery, tsheb thiab structural engineering industries. Nws yog feem ntau siv los thauj cov kua, roj thiab cov khoom khib nyiab nyob rau hauv qhov kub siab thiab kub ib puag ncig. Qhov no ntau yam tubing yog siv nyob rau hauv pipelines, roj qhov dej, hydraulic systems, mechanical Cheebtsam, thiab lwm yam kev siv uas yuav tsum tau txhim khu kev qha, npaum cov ntaub ntawv hloov.

Lub tuam txhab cov khoom zoo zoo:

High-Quality Manufacturing: Peb 40MnB carbon steel seamless kav yog tsim los ntawm advanced manufacturing cov tswv yim los xyuas kom meej meej thiab niaj hnub qhov ntev nrog zoo heev sab hauv thiab sab nrauv tiav.
Kev Tswjhwm nruj nruj: Peb ua raws li kev tswj xyuas nruj nruj thoob plaws hauv cov txheej txheem tsim khoom kom ntseeg tau tias peb cov kav dej steel ua tau raws li cov qauv kev lag luam.
Kev xaiv cov khoom zoo: Peb tau txais cov khoom zoo 40MnB carbon steel, paub txog nws lub zog zoo dua thiab ua haujlwm ntev, los xyuas kom meej lub neej kev pabcuam thiab kev ua haujlwm ntawm cov kav dej seamless.
Superior Performance: Peb 40MnB carbon steel seamless kav muab zoo heev hardness, hnav tsis kam thiab kev ntseeg siab rau kev thov kev lag luam.
Custom Options: Peb muab cov kev cai xaiv hauv qhov loj, ntev thiab ua tiav kom tau raws li qhov yuav tsum tau ua.

Pab Pawg Qhia

40MnB Carbon Steel Seamless Pipe