API 5l X60 Seamless Yeeb Nkab
API 5l X60 Seamless Yeeb Nkab
video
API 5l X60 SMLS Steel Pipe
API 5l X60 Carbon Seamless Pipe
API 5l X60 Seamless Steel Tube
1/2
<< /span>
>

API 5l X60 Seamless Yeeb Nkab

API 5l x60 seamless steel yeeb nkab yog ua los ntawm cov pa roj carbon zoo yog li nws muaj zog, ruaj thiab corrosion resistant. Nws cov seamless kev tsim kho kuj ua kom lub ntsej muag du, uas txo cov kev sib txhuam thiab tso cai rau cov kua dej ntws zoo thiab ua tau zoo los ntawm cov yeeb nkab.

 

API 5L X60 Seamless Steel Pipe Supplier-GNEE

Khoom Description

API 5L X60 yeeb nkab yog muaj nyob rau sab nraud diameters li ntawm ½ "mus rau 100" thiab muaj qhov tsawg kawg nkaus lub zog ntawm 415 MPa. API qib 5L X60 kav dej muaj ob theem, PSL1 thiab PSL2. API Qib 5L X60 yeeb nkab muaj lub zog tensile siab, ua rau nws ruaj khov, ua haujlwm siab thiab muaj peev xwm tiv taus siab.

Txuj
API 5L,API 5 CT, ASTM A106 1/A53, ASTM A519 Cov Lus Qhia Tshwj XeebJIS G 3441, JIS G3444, JIS G3445, DIN 2391, EN10305, EN10210, ASME SA106, SA192 SA210, SA213, SA335, DIN17175, ASTM A179
Tawm Dia
10 3- 1016mm
Phab ntsa Thickness
1 0-100 hli
Cov yeeb nkab ntev
Tsau ntev, random ntev SRL, DRL lossis raws li xav tau
Khoom siv
ASTM A106 carbon seamless steel yeeb nkab
Qib Steel
API 5L, GR B, X42, X46, X56, X60, X65, X70
ASTM A53.A106: GR A, GR B, GR C
ASME SA106: GR. A, GRB, GR.C
ASME SA192: SA192
ASME SA209M: T1, T1a
ASME SA210: GR.AQ, GR.C
ASME SA213: T2, T5, T9, T11, T12, T22
ASME SA335: P2, P5, P9, P11, P12, P22, P91
DIN7175: ST35.8, ST45.8, 15Mo3, 13CrMo44
Kev kho cua sov
Annealed: Ci ntsa iab, Spheroidize annealed, Normalized, Stress relieved, txias tiav, quenched thiab tempered
Nto
Dub xim, kua roj vanish, roj, galvanized
Xaus tiv thaiv
1. Cov kaus mom yas (OD me)
 
2. Hlau tiv thaiv (loj OD)
Daim ntawv thov
Cov yeeb nkab dej, roj yeeb nkab, cov yeeb nkab roj, cov yeeb nkab, cov yeeb nkab boiler
Kuaj
Chemical Component Analysis, Mechanical Properties, Technical Properties, External Size Inspection, Hydrostatic Test, X-ray Test.
Lus ceeb toom
Tsim tshwj xeeb muaj raws li qhov yuav tsum tau ua

API 5l X60 Seamless Carbon yeeb nkab

API 5l x60 Pipe

Api 5l X60 Yeeb Nkab Khoom Sib npaug

ASTM API 5L Cov Lus Qhia Specification rau kab yeeb nkab
Khoom Qib PSL1 l415x 60
Khoom Qib PSL2 L415N or X60 N
L415Q or X60 Q
L415M or X60M

 

Tshuaj Resistance Guide Ntawm Api 5l X60 Kab Yeeb

X60 PSL1 X60 PSL 2

Qib

Mn (siab tshaj)

C (siab tshaj)

P (siab tshaj)

C (siab tshaj)

S (siab tshaj)

P (siab tshaj)

Mn (siab tshaj)

S (siab tshaj)

X60

1.040

0.026

0.003

0.022

0.003

0.0025

1.045

0.0015

 

API 5L X60 SMLS Properties

API 5L Gr.B X60 PSL 1 Mechanical Properties
Qib Yield zog Mpa Tensile zog Mpa Elongation
B 245 415 c
X60 415 520 c

 

API 5L X60N / X60Q PSL 2 Mechanical Properties
Qib Yield zog Mpa Tensile zog Mpa Raito Elongation
  min max min max max min
BN 245 450 415 655 0.93 f
BQ
X60N 415 565 520 760 0.93 f
X60Q

 

FAQ

Q. Koj lub warranty ntev npaum li cas?
A: Peb lub sijhawm lav yog 12-36 hli, lub sijhawm tshwj xeeb nyob ntawm cov khoom.
Q. Kuv puas tuaj yeem tau txais cov qauv dawb?
A: Yog, peb tuaj yeem muab cov qauv dawb rau koj, tab sis koj yuav tsum tau them tus nqi thauj khoom los ntawm koj tus kheej.
Q. Kuv puas tuaj yeem thov hloov daim ntawv ntim thiab xa khoom?
A: Yog, peb tuaj yeem hloov daim ntawv ntim thiab xa khoom raws li koj xav tau, tab sis koj yuav tsum tau them tus nqi thiab tus nqi sib txawv thaum lub sijhawm no.
Q. Kuv puas tuaj yeem thov kev xa khoom sai?
A: Yog lawm, peb yuav npaj rau koj API 5l X60 smls yeeb nkab kom sai li sai tau.