ASTM A106 A210 A333 Seamless Steel Yeeb Nkab

ASTM A333 yog seamless carbon steel yeeb nkab haum rau qhov kub thiab txias. ASTM A106 seamless steel yeeb nkab belongs rau American standard steel yeeb nkab. A106 suav nrog A106-A thiab A106-B. Nws belongs rau cov pa roj carbon zoo tib yam series thiab yog ib qho ntawm cov khoom siv feem ntau. A210 yog ib qho kev qhia tshwj xeeb rau nruab nrab carbon steel seamless steel kav rau boilers thiab superheaters, suav nrog Qib a -1 thiab Qib C.

 

Carbon Seamless Steel Yeeb Nkab Supplier-GNEE

A106 A333 A210 Seamless Steel Pipe Description

ASTM A106, A210, thiab A333 yog tag nrho cov qauv siv dav rau cov kav dej seamless hauv kev lag luam. Cov kav dej no paub txog lawv cov kev ua haujlwm siab, ua haujlwm ntev, thiab lub zog. Qib A106 yog tsim los rau kev siv kub thiab siab thiab siv hauv kev lag luam roj, roj, thiab dej. Qib A210 tshwj xeeb yog pom zoo rau chav boilers thiab superheater raj. A333 qib yog tsim los rau cov ntawv thov kub thiab feem ntau siv hauv kev lag luam xws li roj thiab roj thiab petrochemicals.

Daim ntawv thov

Petroleum, Tshuaj lom neeg kev lag luam, khoom siv kho tshuab

Kev Pabcuam

Bending, Vuam, Decoiling, Punching, Txiav, Moulding

Ntim

Txheem Seaworthy Pob, raws li cov neeg siv khoom xav tau

MOQ

30 TON

Nto

Annealed, pickled, polished

 

ASTM A106 Seamless Carbon Steel Yeeb Nkab Cov Kev Xav Tau

 

Kev sib xyaw,%
Qib A Qib B Qib C
Cov pa roj carbon, maxA 0.25 0.30 0.35
Manganese 0.27-0.93 0.29-1.06 0.29-1.06
Phosphorus, max 0.035 0.035 0.035
Sulfer, max 0.035 0.035 0.035
Silicon, min 0.10 0.10 0.10
Chrome, maxB 0.40 0.40 0.40
tooj liab, maxB 0.40 0.40 0.40
Molybdenum, maxB 0.15 0.15 0.15
Nickel, maxB 0.40 0.40 0.40
Vanadium, maxB 0.08 0.08 0.08

 

ASTM A210 Carbon Steel Tube Chemical Composition

Qib

C (Max) Mn Si (Min) P (Max)

S (Max)

A1

0.27 Max 0.93 0.10 0.035 0.035
C 0.35 0.29~1.06 0.10 0.035

0.035

 

ASTM A333 Steel Pipe Chemical Composition:

Txuj Qib Chemical Composition (%)
C Si Mn P S Cr Ni Cu Mo V Al
ASTM A333 Cov khoom lag luam Qib 1 Tsawg dua lossis sib npaug rau 0.30   0.40~1.06 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.025            
Qib 3 Tsawg dua lossis sib npaug rau 0.19 0.18~0.37 0.31~0.64 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.025   3.18~3.82        
Qib 4 Tsawg dua lossis sib npaug rau 0.12 0.18~0.37 0.50~1.05 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.025 0.44~1.01 0.47~0.98 0.40~0.75     0.04~0.30
Qib 6 Tsawg dua lossis sib npaug rau 0.30 Ntau dua lossis sib npaug rau 0.10 0.29~1.06 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.025            
Qib 7 Tsawg dua lossis sib npaug rau 0.19 0.13~0.32 Tsawg dua lossis sib npaug rau 0.90 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.025   2.03~2.57        
Qib 8 Tsawg dua lossis sib npaug rau 0.13 0.13~0.32 Tsawg dua lossis sib npaug rau 0.90 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.025   8.40~9.60        
Qib 9 Tsawg dua lossis sib npaug rau 0.20   0.40~1.06 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.025   1.60~2.24 0.75~1.25      
Qib 10 Tsawg dua lossis sib npaug rau 0.20 0.10~0.35 1.15~1.50 Tsawg dua lossis sib npaug rau 0.03 Tsawg dua lossis sib npaug rau 0.015 Tsawg dua lossis sib npaug rau 0.15 Tsawg dua lossis sib npaug rau 0.25 Tsawg dua lossis sib npaug rau 0.015 Tsawg dua lossis sib npaug rau 0.50 Tsawg dua lossis sib npaug rau 0.12 Tsawg dua lossis sib npaug rau 0.06
Qib 11 Tsawg dua lossis sib npaug rau 0.10 Tsawg dua lossis sib npaug rau 0.35 Tsawg dua lossis sib npaug rau 0.6 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.025 Tsawg dua lossis sib npaug rau 0.50 35.0~37.0   Tsawg dua lossis sib npaug rau 0.50    

 

ASTM A106 A210 A333 Yeeb Nkab

ASTM A106 A210 A333 Seamless Steel Pipe Supplier

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Cov lus pom zoo

A333 Qib 6 Tsawg Carbon Steel Pipes

ASTM A210 A333 Seamless Steel Yeeb Nkab

SA106 B Carbon Steel Yeeb Nkab

 

FAQ:

Q1: Koj lub sijhawm xa khoom yog dab tsi?
A: Peb tuaj yeem xa nws hauv 30 hnub tom qab tau txais qhov tso nyiaj.
Q2: Kuv puas tuaj yeem tso tus qauv txiav txim thiab koj tus MOQ yog dab tsi yog tias kuv lees txais koj qhov zoo?
A: Yog lawm, peb tuaj yeem xa cov qauv tuaj rau koj tab sis koj tuaj yeem them tus nqi nthuav dav thiab cov qauv customized yuav siv li ntawm 5-7 hnub, peb MOQ yog 1 tuj.
Q3: Koj tuaj yeem lav koj cov khoom li cas?
A: Mill Test Certification yog muab nrog cov khoom xa tuaj, Peb kuj lees txais thiab txhawb nqa qhov kev tshuaj xyuas thib peb. Peb kuj tuaj yeem muab qhov warranty rau cov neeg siv khoom kom lav qhov zoo.
Q4: Kuv tuaj yeem tau txais tus nqi ntawm cov khoom xav tau li cas?
A: Nws yog txoj hauv kev zoo tshaj yog tias koj tuaj yeem xa peb cov khoom, qhov loj thiab qhov chaw, yog li peb tuaj yeem tsim rau koj los xyuas qhov zoo. Yog tias koj tseem muaj qhov tsis meej pem, tsuas yog tiv tauj peb, peb xav pab.
 

Cim npe nrov: astm a106 a210 a333 seamless steel yeeb nkab, Tuam Tshoj astm a106 a210 a333 seamless steel yeeb nkab manufacturers, lwm tus neeg, Hoobkas