T22 Seamless Steel Yeeb Nkab
Peb lub chaw tsim khoom lag luam niaj hnub siv cov thev naus laus zis thev naus laus zis thiab cov tshuab muaj peev xwm ua tau raws li T22 Seamless Steel Tubes. Peb ua qhov tseem ceeb ntawm kev tswj hwm kev ua tau zoo thiab ua raws li cov cai hauv kev lag luam.
T22 Seamless Steel Yeeb Nkab
T22 Seamless Steel Tube yog qib siab steel raj tsim los rau ntau hom kev lag luam. Crafted nrog precision kws txawj, no seamless steel raj muaj exceptional durability, kev cia siab rau thiab efficiency. Ua los ntawm cov cuab yeej siv siab heev thiab cov khoom siv zoo, nws yog qhov zoo tagnrho rau kev xav tau ib puag ncig.
T22 Seamless Steel Pipe Description
|
yam |
tus nqi |
|
Daim ntawv thov |
Fluid Pipe, Boiler Pipe, Gas Pipe, OIL PIPE |
|
Alloy Los Tsis |
Tsis-Alloy |
|
Tshooj Duab |
Hloov |
|
Thickness |
0 8 - 12.75 hli |
|
Txuj |
EN, BS, JIS, thiab lwm yam |
|
Ntev |
12M, 6m, 6.4M |
|
Daim ntawv pov thawj |
API, ce, Bsi, BIS, JIS, GS, ISO9001 |
|
Cov txheej txheem |
ERW |
|
Kev Pabcuam |
Vuam, Punching, txiav, dabtsi yog khoov |
|
Invoicing |
los ntawm theoretical hnyav |
|
Lub sij hawm xa tuaj |
7-15 hnub |
|
Ntev |
Customized |
|
Thickness |
0 55-20mm |
|
MOQ |
5 Tons |
|
Cov nqe lus them nqi |
30 feem pua TT Ua ntej ntxiv rau 70 feem pua Sij hawm |
|
Qib Steel |
Q195-Q235/st 37/52 |
|
Xim |
Dub....raws li cov neeg siv khoom xav tau |
|
Cov cim |
raws li cov neeg siv khoom xav tau |
|
Qauv |
Qauv Dawb |

Product Mechanical Performance Table:
| Khoom | Tus nqi |
|---|---|
| Tensile zog | Ntau dua lossis sib npaug li 415 MPa |
| Yield zog | Ntau dua lossis sib npaug li 205 MPa |
| Elongation | Ntau dua lossis sib npaug li 30 feem pua |
| Hardness (HRB) | Tsawg dua lossis sib npaug li 85 HRB |
Khoom zoo
Cov khoom siv zoo heev: lub zog tensile siab thiab lub zog tawm los, tuaj yeem tiv taus qhov hnyav thiab siab.
Smooth Surface: Kev sib txhuam yam tsawg kawg nkaus, zoo tagnrho rau kev hloov pauv cov kua thiab roj.
High Temperature Resistance: Ua kom muaj kev ntseeg ruaj khov ntawm qhov kub siab.
Corrosion kuj: Haum rau corrosive ib puag ncig, ua kom lub neej ntev ntawm cov khoom.
Formability: Ib qho yooj yim rau daim ntawv thiab lis rau tej daim ntaub ntawv.
Solderability muab zoo heev solderability rau kev koom tes thiab fabrication.
Uniform Composition: Cov khoom siv sib xyaw ua ke kom ntseeg tau tias kev ua tau zoo.
Versatility: Haum rau kev lag luam xws li petrochemical, tsim hluav taws xob thiab kev tsim kho.
Pab pawg tuam txhab

Tuam txhab Hoobkas

Cim npe nrov: t22 seamless steel yeeb nkab, Tuam Tshoj t22 seamless steel yeeb nkab manufacturers, lwm tus neeg, Hoobkas