TP304 Seamless Steel Square Tube
TP304 stainless hlau yeeb nkab yog cov khoom siv hlau tsis zoo uas feem ntau siv nrog kev tiv thaiv corrosion zoo thiab kev ua haujlwm kub, uas yog siv dav hauv cov kav dej xa dej thiab cov hlab ntsha siab hauv cov roj av, tshuaj, khoom noj, tshuaj, thiab lwm yam. Cov txheej txheem tsim khoom ntawm TP304 stainless hlau yeeb nkab feem ntau suav nrog ob txoj hauv kev kub-kuav los tiag thiab txias-kuav los tiag, nyob rau hauv uas txias-dov TP304 stainless hlau yeeb nkab muaj qhov tseeb dua qhov ntev thiab lub ntsej muag smoother, thiab yog li ntawd ntau dav siv nyob rau hauv high-end teb.
TP304 Seamless Steel Tube
TP304 Seamless Square Steel Tube
Qhov kev pabcuam kub ntawm TP304 stainless hlau seamless yeeb nkab tuaj yeem ncav cuag 650 degrees Celsius, thiab tiv thaiv oxidation kub tuaj yeem ncav cuag li 850 degrees Celsius. Siv nyob rau hauv manufacturing loj generator teem boiler superheater hlab, reheater raj, chav kav, thiab tshav kub exchangers raj nyob rau hauv lub petrochemical kev lag luam
Khoom Description
|
Khoom npe |
TP304 Square Seamless Steel Tube |
|
Ntev |
Raws li xav tau |
|
Qib hlau |
300 series |
|
Thickness |
0 5-100mm los yog raws li xav tau |
|
Txuj |
ASTM A213, A312, ASTM A269, ASTM A778, ASTM A789, DIN 17456, DIN17457, DIN 17459, JIS G3459, JIS G3463, GOST 9941, EN10216, BS3269, |
|
Cov txheej txheem |
Kub Rolled, Txias Rolled, Extrusion |
|
Nto |
Polishing |
|
Thickness kam rau ua |
± 0.01 hli |
|
Khoom siv |
304, 304L, 309S, 310S, 316,316Ti, 317,317L, 321,347,347H, 304N, 316L, 316N, 201,202 |
|
Daim ntawv thov |
Siv dav hauv roj av, khoom noj khoom haus, tshuaj lom neeg kev lag luam, kev tsim kho, hluav taws xob fais fab, nuclear, zog, tshuab, biotechnology, ntawv ua, nkoj tsim, thiab boiler teb. |
|
MOQ |
30 tons, Peb tuaj yeem txais cov qauv txiav txim. |
|
Lub Sijhawm xa khoom |
Hauv 30 hnub ua haujlwm tom qab tau txais qhov tso nyiaj lossis L / C |
|
Export Ntim |
Txheem seaworthy export packing lossis raws li cov neeg siv khoom thov |
|
Muaj peev xwm |
25000 Tons / Tons ib hlis |
TP304 tuab phab ntsa stainless hlau raj

STAINLESS STEEL SQUARE TUBE CHEMICAL COMPOSITION
| QIB | UNS | C | Mn | P | S | Si | Cr | Ni | Mo | Ti | Nb | N |
| TIAB SA 304 | S30400 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 8.0-11.0 | ||||
| TP 304 L | S30403 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 8.0-13.0 | ||||
| TIAB SA 316 | S3160 | 0.08 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 11.0-14.0 | 2.0-3.0 | |||
| TP 316 L | S31603 | 0.035 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 |
STAINLESS STEEL SQUARE TUBE MECHANICAL PROPERTIES
| Khoom siv | Kub | Kub | Tensile zog | Yield zog | Elongation %, Min |
| Kev kho mob | Min. | Ksi (MPa), Min. | Ksi (MPa), Min. | ||
| º F(º C) | |||||
| TIAB SA 304 | Kev daws | 1900 (1040) | 75(515) | 30(205) | 35 |
| TP 304 L | Kev daws | 1900 (1040) | 70(485) | 25(170) | 35 |
| TIAB SA 316 | Kev daws | 1900(1040) | 75(515) | 30(205) | 35 |
| TP 316 L | Kev daws | 1900(1040) | 70(485) | 25(170) | 35 |
Kev pab cuam tom qab muag:
Peb qhov kev cog lus rau cov neeg siv khoom txaus siab txuas ntxiv dhau qhov kev yuav khoom. Peb muab kev pab cuam tom qab muag, suav nrog:
Kev sib tham tob txog cov khoom lag luam los daws cov lus nug thiab qhia kev teeb tsa.
Kev txhawb nqa kev saib xyuas, kev ua haujlwm, thiab siv cov lus nug.
Warranty npog tiv thaiv kev tsim khoom tsis xws luag.
Xaiv TP304 square yeeb nkab los txhim kho koj qhov project nrog kev sib xyaw ua ke zoo tshaj plaws ntawm lub zog, kev zoo nkauj, thiab kev ua haujlwm ntev. Cov khoom tau ua tib zoo tsim thiab tsim kom tau raws li cov qauv siab tshaj plaws thiab yog ib qho pov thawj rau kev daws teeb meem zoo tshaj plaws.
GNEE Cov neeg siv khoom

GNEE Hoobkas

GNEE Team

Stainless hlau square yeeb nkab tshuaj xyuas

loj txoj kab uas hla steel tubing ntim thiab shipping

Cim npe nrov: tp304 seamless steel square raj, Tuam Tshoj tp304 seamless steel square raj manufacturers, lwm tus neeg, Hoobkas
Xa kev nug