Loj Loj Stainless Hlau Yeeb Nkab 304

Stainless hlau kav yog dav siv nyob rau hauv ntau yam lag luam rau lawv cov durability, corrosion kuj, thiab siab zog zog. Ntawm lawv, txoj kab uas hla loj stainless hlau kav tau dhau los ua neeg nyiam vim lawv muaj peev xwm tuav cov khoom hnyav thiab tiv taus qhov kub thiab txias.

 

Qib 304 Stainless Hlau:

Stainless hlau qib 304, tseem hu ua 18-8 stainless hlau, yog ib qho ntawm feem ntau siv thiab ntau yam stainless hlau qib.

Nws muaj 18-20 feem pua ​​​​chromium thiab 8-10.5 feem pua ​​​​nickel, uas muab kev tiv thaiv corrosion zoo heev, txawm tias nyob hauv ib puag ncig hnyav.

Cov kav dej loj:

Loj txoj kab uas hla stainless hlau kav feem ntau muaj diameters ntau tshaj 2 ntiv tes (50.8 hli). Qhov ntau npaum li cas yuav txawv nyob ntawm tus neeg muag khoom thiab cov chaw tsim khoom.

Daim ntawv thov:

Loj txoj kab uas hla 304 stainless hlau kav pom cov ntawv thov hauv ntau qhov kev lag luam, suav nrog:

Kev tshawb nrhiav thiab kev tsim roj thiab roj

Kev ua tshuaj lom neeg

Kev ua zaub mov thiab dej haus

Kev tsim tshuaj

Kev tsim kho thiab architectural tej yaam num

Automotive thiab kev thauj mus los

Kev kho dej thiab kev faib tawm

Kev tsim khoom siv hluav taws xob

Daim ntawv:

Loj txoj kab uas hla stainless hlau kav muaj nyob rau hauv ntau hom, nrog rau seamless thiab welded kav. Kev xaiv ntawm seamless thiab welded kav yog nyob ntawm cov kev thov tshwj xeeb.

Qhov ntau thiab tsawg:

Cov kav dej loj loj tuaj yeem muaj qhov loj me los ntawm ob peb nti mus rau ob peb taw hauv txoj kab uas hla, nyob ntawm qhov project specifications.

Thickness:

Phab ntsa tuab ntawm txoj kab uas hla loj stainless hlau kav tuaj yeem sib txawv los ua kom tau raws li qhov sib txawv siab thiab cov qauv tsim.

Nto tiav:

Kev ua tiav ntawm cov kav dej no tuaj yeem sib txawv, suav nrog cov kev xaiv xws li pickled, annealed, polished, lossis zeb tiav, nyob ntawm seb qhov xav tau siv thiab cov neeg siv khoom nyiam.

Qauv:

Loj txoj kab uas hla stainless hlau kav yuav tsum ua raws li cov qauv kev lag luam, xws li ASTM A312 (rau seamless thiab welded kav) los yog ASTM A358 (rau hluav taws xob-fusion-welded kav).

Muaj:

Koj tuaj yeem tau qhov loj txoj kab uas hla 304 stainless hlau kav los ntawm ntau yam stainless hlau lwm tus neeg thiab manufacturers. Nws yog ib qho tseem ceeb uas yuav tau xaiv ib tus neeg muag khoom muaj npe nrov uas tuaj yeem muab cov kav dej uas ua tau raws li koj cov kev xav tau tshwj xeeb thiab cov qauv zoo.

Tus nqi:

Tus nqi ntawm txoj kab uas hla loj stainless hlau kav yuav txawv nyob ntawm seb qhov loj me, phab ntsa thickness, kom muaj nuj nqis, zoo, thiab kev ua lag luam.

Hom kev sib txuas Vuam
Specification GB, DIN, JIS, EN, ASTM
Hla-Section Shape Hloov
Thauj Pob Seaworthy Ntoo Cases / Plywood Cases / hauv Bundles
Muaj Peev Xwm Ntau Lawm 1000mt / hli

product-911-750

FAQ:

Q1: Koj puas tuaj yeem muab cov qauv?
A: Nco ntsoov tus phooj ywg, peb tuaj yeem muab cov qauv dawb ntawm cov xwm txheej uas nws muaj nyob hauv cov khoom lag luam, txawm li cas los xij, tus nqi thauj mus los yog tus neeg yuav khoom.


Q2: Koj puas txais OEM, ODM?
A: Tseeb. Yog tias tsim nyog, peb tuaj yeem ntxiv koj lub logo rau ntawm cov khoom.


Q3: Yuav ua li cas txog cov nqe lus them nqi?
A: Raws li daim ntawv cog lus.
 