ASTM A691 steel yeeb nkab
ASTM A691 steel yeeb nkab
video
ASTM A691 Alloy Steel EFW Pipe
A691 Chrome Moly Alloy Welded Pipe
A691 alloy steel pipe
1/2
<< /span>
>

ASTM A691 steel yeeb nkab

MOQ: 30 Tuj
Lub sij hawm xa tuaj: 30 hnub
Tshooj Shape: Round

 

Product Description

ASTM A691 yeeb nkab yog electrofusion welded specification yeeb nkab. Cov kav dej no muaj nyob rau hauv qhov loj dua li ntawm 16 ntiv mus rau 100 ntiv tes. A691 yeeb nkab yog carbon hlau nrog phosphorus, sulfur, manganese, thiab carbon nyob rau hauv nws muaj pes tsawg leeg. Muaj qhov sib txawv ntawm cov qib. ASTM A691 cov kav dej yog tsim los ntawm cov hlau-raws li alloy uas muaj ntau qib ntawm chromium, molybdenum, thiab lwm yam. Qhov kev sib xyaw ua ke no ua rau lawv tsis tshua muaj zog thiab corrosion resistant. Lawv lub zog yog ntxiv los ntawm austenitic grain loj ntawm Rockwell hardness 5 los yog finer. Vim nws lub zog zoo dua thiab ua haujlwm ntev, ASTM A691 alloy steel yeeb nkab muaj ntau yam kev siv hauv kev lag luam xws li petrochemical processing thiab pipeline tsim.

Hlau Yeeb Nkab ASTM A691 Specification

Txuj

ASTM, AISI, SUS, JIS, EN, DIN, BS, GB, thiab lwm yam.

Khoom siv

Q235, Q195, Q345, SPCC, SPCD, SPCE, SPCEN, ST12, ST13, ST14, ST15, ST16.

DC01, DC03, DC04, DC05, DC06

Txoj kab uas hla

1/2" -12" (21.3-323.9mm)

Thickness

{{0}} 8-10.0mm, Raws li Koj Qhov Kev Thov

Ntev

6. 0M, 6.5M, 5.0M, 4.0M, 3. los ntawm cov neeg siv khoom xav tau

International Standard

ISO 9000-2001, CE CERTIFICATE, BV CERTIFICATE

Yam khoom

Metallurgy, Mineral & Zog

Cov txheej txheem

Welded

Kev lag luam loj

Middle East, Africa, Asia thiab qee lub tebchaws Uropean thiab South America, Australia

A691 Chrome Moly Alloy Welded Yeeb Nkab

sp38

ASTM A 691 1-1/4CR Cov Yeeb Nkab Tshuaj Muaj Zog

ASTM A691 Cov Lus Qhia Tshwj Xeeb Qib 1 1/4CR
C 0.05-0.17
Mn 0.40-0.65
P 0.025
S 0.025
Si 0.50-0.80
Cr 1.00-1.50
Mo 0.45-0.65

FAQ

1. Q: Koj puas xa tuaj raws sijhawm?
A: Yog, peb tau cog lus los muab cov khoom zoo tshaj plaws thiab xa lawv raws sijhawm. Kev ncaj ncees yog lub hauv paus ntsiab lus ntawm peb lub tuam txhab.
2. Q: Koj puas muab cov qauv? Puas yog lawv pub dawb lossis ntxiv?
A: Cov qauv tuaj yeem muab pub dawb rau cov neeg siv khoom, tab sis tus nqi xa khoom xa tuaj yuav raug them los ntawm tus neeg siv khoom tus account.
3. Q: Koj puas lees txais kev tshuaj xyuas thib peb?
A: Yog, peb lees txais nws kiag li.
4. Q: Koj tuaj yeem lav koj cov khoom li cas?
A: Txhua yam khoom yog tsim nyob rau hauv ib lub rhiav ntawv pov thawj thiab tshuaj xyuas ib thooj los ntawm QC raws li lub teb chaws QA / QC qauv. Peb tseem tuaj yeem muab warranty rau peb cov neeg siv khoom kom ntseeg tau qhov zoo.

Cim npe nrov: Tuam Tshoj steel yeeb nkab astm a691 manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

(0/10)