ASTM A512 Mechanical Tube
A512 steel tubes yog siv los tswj cov pa roj carbon steel txias kos steel hlab. Cov kav dej no feem ntau siv hauv kev siv tshuab, tsheb thiab engineering.
ASTM A512 Hlau Tube
ASTM A512 steel yeeb nkabyog cov khoom siv carbon steel nrog ib qho tshwj xeeb muaj pes tsawg leeg thiab ntau yam ntawm cov khoom siv kho tshuab. Nws muaj pes tsawg leeg yog carbon (C) {{{0}}}07-0.13, silicon (Si) 0.07-0.37, manganese (Mn) {{ 9} }. , chromium (Cr) Tsawg dua lossis sib npaug 0.15, tooj liab (Cu) Tsawg dua lossis sib npaug rau 0.250, molybdenum (Mo) thiab vanadium (V) txwv. A512 steel yeeb nkab txais cov txheej txheem tsim khoom txias, thiab nws cov qauv sab hauv tau txhim kho los ntawm kev ncab thiab ua haujlwm txias. Qhov txheej txheem tsim qauv ua rau cov qauv cryster crystal ntawm lub raj, ua kom tau zoo txhim kho cov khoom siv cov khoom siv mechanical.
Cov khoom siv ntawm ASTM A512 welded steel yeeb nkab suav nrog tensile zog (MPa) Ntau dua lossis sib npaug ntawm 379, yield zog (MPa) Ntau dua lossis sib npaug rau 241, thiab elongation (%) Ntau dua lossis sib npaug rau 32. Cov txiaj ntsig no qhia tias cov yeeb nkab steel muaj lub zog siab thiab zoo plasticity, tuaj yeem tiv taus cov tensile loj, thiab tswj tau zoo ductility.
ASTM A512 steel yeeb nkab muaj qhov hardness ntawm kwv yees li 55 HRB, qhia tias muaj zog dua thiab hnav zoo dua. thiab cov ntsiab lus vanadium tsis tau hais. Qhov kev faib ua feem ntawm cov ntsiab lus no txiav txim siab lub cev thiab lub zog ntawm cov yeeb nkab steel. Cov yeeb nkab steel zoo li no yog tsim rau ntau yam qauv thiab cov khoom siv xws li cov tsev, txuas hniav, cov kav dej, thiab lwm yam, thiab muaj kev tiv thaiv corrosion zoo thiab lub zog siab.
Khoom Khoom
ASTM A512 Tubing Standard Dimensional Tolerances - Round Tubing
|
Ntev Ntau |
OD Qhov Loj Loj |
Ua siab ntev |
|
4 thiab tsawg |
rau 2 000 |
+1/16-0 |
|
4 thiab tsawg |
2.001 Nws |
+3/32-0 |
|
4 rau 10 |
rau 2 000 |
+3/32-0 |
|
4 rau 10 |
2.001 Nws |
+1/8 -0 |
|
Tshaj 10 |
Tag nrho |
+1/8 -0 |
thaj tsam
Qhov kev qhia tshwj xeeb no suav nrog txias-dhau taub qab-welded carbon steel yeeb nkab siv los ua cov tubing tshuab.
Qhov kev qhia tshwj xeeb no suav nrog puag ncig, square, duab plaub, thiab tshwj xeeb zoo li tus neeg kho tshuab raj.
Round tube loj npaum li cas them yog mus txog {{0}}/2 in. (88.9 mm) sab nraud txoj kab uas hla thiab 0.035 txog 0.500 in. (0.89 mus rau 12.70 mm) phab ntsa tuab.
| Mechanical cwj pwm Lub tensile kev nyuaj siab ntawm round raj mandrel tau raug tshem tawm * |
||||
|
Qib |
Yam tsawg kawg nkaus |
Yam tsawg kawg nkaus |
Elongation |
Yam tsawg kawg nkaus |
|
C-1010 |
58,000 |
63,000 |
15 |
70 |
|
C-1012 |
58,000 |
63,000 |
15 |
70 |
|
C-1015 |
60,000 |
66,000 |
14 |
72 |
|
C-1016 |
61,500 |
67,000 |
13 |
73 |
|
C-1018 |
62,500 |
68,000 |
13 |
73 |
|
C-1020 |
65,000 |
71,000 |
11 |
73 |
|
C-1030 |
70,000 |
80,000 |
10 |
80 |
|
C-1110 |
58,000 |
63,000 |
15 |
70 |
|
C-1115 |
62,500 |
68,000 |
13 |
73 |
* Mos thiab nruab nrab annealed tubing kuj muaj.
ASTM A512 Steel Tube Chaw tsim tshuaj paus

ASTM A512 Tubing Muaj Nto Ua tiav
Nto Finishes: Liab qab, Oiled, Mill Varnish, Galv, FBE, FBE Dual, 3LPE, 3LPP, Coal Tar, Qhob Txheej thiab daim kab xev qhwv.
Xaus Finishes: Beveled, Square Cut, Threaded & Coupled.

Hais txog GNEE
GNEE muaj 12 cov kab ntau lawm nrog cov zis txhua xyoo ntawm 50, 000 tons. Tau txais daim ntawv pov thawj ISO9001 thoob ntiaj teb kev tswj hwm zoo. Nrog kev muag khoom ntau thiab cov khoom muag. Tam sim no warehouse cov lus nug yog ntau tshaj 1,500 tons thiab ntau tshaj 800 specifications. Ua tsaug rau kev tswj xyuas kom zoo thiab xav txog kev pabcuam rau cov neeg siv khoom.Tiv tauj peb tam sim no.

GNEE Cov neeg muas zaub

GNEE Exhibition

Kev tshuaj xyuas yeeb nkab

Ntim thiab shipping

FAQ
Q: Koj puas tuaj yeem muab qhov kev pabcuam?
A. Peb tuaj yeem muab cov khoom siv hlau thiab cov khoom, thiab peb kuj tuaj yeem muab lwm cov kev pabcuam.
Q: Kuv puas tuaj yeem tau txais cov qauv ua ntej xaj?
A: Yog lawm, tau kawg. Feem ntau, peb cov qauv pub dawb. peb tuaj yeem tsim koj cov qauv lossis kos duab kos duab.
Koj ua li cas xyuas tag nrho cov khoom hauv cov kab ntau lawm?
A: Peb muaj cov chaw soj ntsuam thiab kuaj cov khoom tiav. Peb xyuas cov khoom thaum lawv mus rau hauv cov txheej txheem ntau lawm tom ntej.
Qhov txawv ntawm A512 thiab A513 yog dab tsi?
A.ASTM A513 tau teev tsegrau Resistance Welded (ERW) carbon thiab alloy Electric mechanical tubing, thaum ASTM A512 npog txias-draw buttweld carbon steel mechanical tubing,
Cim npe nrov: ASTM A512 Mechanical Tube, Tuam Tshoj ASTM A512 Mechanical Tube manufacturers, lwm tus neeg, Hoobkas
Xa kev nug