ASTM A36 Carbon Steel Welded Yeeb Nkab
A36 carbon structural vaj huam sib luag yog tus qauv Asmeskas tau teev tseg hauv ASTM A36. Cov qauv no siv rau riveted, bolted thiab welded qauv rau txuas hniav thiab cov tsev, thiab rau carbon steel seem, daim hlau thiab tuav rau cov qauv steel. A36 yog cov feem ntau siv kub dov carbon structural steel. Nws muaj qhov tsawg kawg nkaus lub zog ntawm 36k psi thiab yog yooj yim weldable.
ASTM A36 Hlau Welded Yeeb Nkab
ASTM A36 Carbon Steel Welded Yeeb Nkab
A36 steel yog cov khoom siv carbon steel siv hauv kev tsim cov welded thiab bolted hlau cov qauv hauv kev lag luam thiab pej xeem cov tsev thiab kev tsim choj. ASTM A36 steel kuj tseem siv los tsim cov khoom lag luam thiab cov khoom siv rau kev tsim kho thiab siv tshuab engineering.
ASTM A36 Carbon yeeb nkab

| Cov qib steel |
Q195, Q235A-B, Q345A-E, 20#, 10#,16 MnTxheem: ASTM A36, ASTM A500, ASTM A53, ASTM 106, SS400, St37, St52, S235JR, S355TRH thiab lwm yam. |
||
| Cov qauv | GB/T 3091-2001, GB/T13912-2002, BS 1387, ASTM F1083 thiab lwm yam. | ||
| Cov yeeb nkab kawg |
Plain, beveled, threaded, socket nrog qhov, nrog PVC clap / coupling / clamp, los yog raws li cov neeg siv khoom xav tau |
||
| kev kho mob | |||
| Daim ntawv thov |
Kev xa tawm ua kua (twj dej, roj, dej, roj), kev tsim cov yeeb nkab, kev tsim kho yeeb nkab (tsev cog khoom, laj kab ncej), kab hlau rhuav phab ntsa, machinery feem ect. |
||
| Pob |
nyob rau hauv pob, tsis muaj lwm yam pob los yog qhwv nrog waterproof, los yog raws li cov neeg siv khoom xav tau |
||
| Lub sij hawm xa tuaj | 10 hnub los ntawm Tshuag; 15-25 hnub ua raws li qhov qty | ||
| Them Nyiaj | T / T lossis L / C | ||
| Nqe Nqe | CIF; CFR; FOB | ||
| Chaw thau khoom chaw nres nkoj | Qingdao Tianjin lossis Shanghai chaw nres nkoj hauv Suav teb | ||
| Lwm tus |
1.Tag nrho cov kav dej yog high-frequency welded. 2. Ob sab hauv thiab sab nraud welded stab tuaj yeem raug tshem tawm. 3.Kev tsim tshwj xeeb muaj raws li qhov yuav tsum tau ua. 4. Cov yeeb nkab tuaj yeem ua rau caj dab thiab punched qhov. 5.Supplying BV lossis SGS Inspection yog tus neeg xav tau. |
||
ASTM A36 Cov Khoom Siv Tshuaj:
| C | Si | Mn | P | S | Cu (Thaum muaj tooj liab tau teev tseg) |
| Tsawg dua lossis sib npaug li % | Tsawg dua lossis sib npaug li % | % | Tsawg dua lossis sib npaug li % | Tsawg dua lossis sib npaug li % | Ntau dua lossis sib npaug li % |
| 0.25 | 0.4 | 0.80-1.20 | 0.04 | 0.05 | 0.20 |
ASTM A36 Lub cev muaj zog:
| Qib | Specification | ASTM A36 Qib A | ASTM A36 Qib B | ASTM A36 Qib C |
| ASTM A36 | Lub zog tensile, min, psi (MPa) | 48000(330) | 60000(415) | 70000(485) |
| Yield zog, min, psi (MPa) | 30000(205) | 35000(240) | 40000(275) |
FAQ
Q: Koj tus nqi yog dab tsi?
A: Peb cov nqi sib tw heev vim peb yog lub Hoobkas. Yog tias koj txaus siab rau peb cov khoom, thov koj xav tiv tauj peb.
Q: Kuv tuaj yeem tuaj xyuas koj lub Hoobkas?
A: Tau kawg, peb yuav npaj cov neeg ua haujlwm tshaj lij los nrog koj ntawm koj txoj kev taug kev tom qab koj lees paub koj qhov kev taug kev.
Q: Cov ntaub ntawv khoom dab tsi kuv yuav tsum tau muab?
A: Koj yuav tsum tau muab qib, dav, tuab, txheej thiab tonnage yuav.
Q: Cov khoom puas tau kuaj xyuas ua ntej xa khoom?
A: Tau kawg, tag nrho peb cov khoom raug soj ntsuam nruj ua ntej ntim, thiab cov khoom tsis tsim nyog yuav raug rhuav tshem. Peb lees txais kev tshuaj xyuas thib peb.
Q: Lub sijhawm khoom xa tuaj ntev npaum li cas?
A: Tsis pub dhau 7-21 hnub tom qab peb lees paub koj qhov kev thov.
Q: Txoj kev them nyiaj yog dab tsi?
A: Peb lees txais T / T, 100% L / C (them ntawm pom), nyiaj ntsuab, Western Union, yog tias koj muaj lwm txoj kev them nyiaj, thov hu rau kuv.
PEB TEAM

Peb lub Hoobkas

Cim npe nrov: ASTM A36 Carbon Steel Welded Yeeb Nkab, Tuam Tshoj ASTM A36 Carbon Steel Welded yeeb nkab manufacturers, lwm tus neeg, Hoobkas
Xa kev nug