Cov Khoom Siv Uas Muaj:
Grey cam khwb cia hlau
Siv rau media (dej, chav dej, huab cua, roj av, roj) ntawmPn tsawg dua los yog sib npaug rau 1.0 MPA, Kub: -10 Qib rau 200 degree.
Cov qib kawm:HT200, HT250, HT300, HT350.
Mallable cam khwb cia hlau
Siv rau media (dej, chav dej, huab cua, roj) ntawmPn tsawg dua los yog sib npaug rau 2.5 MPA, kub: -30℃mus rau 300 degree.
Cov qib kawm:Kth300-06, Keth330-08, Kth350-10.
Zas Hlau
Siv rau media (dej, chav dej, huab cua, roj) ntawmPn tsawg dua los yog sib npaug rau 4.0 MPa, Kub: -30 Qib rau 350 Qib.
Cov qib kawm:QT400-15, Qt450-10, Qt500-7.
Acid -} tiv taus siab siab- tsov ntxhuav hlau
Siv rau corrosive media ntawmPn tsawg dua los yog sib npaug rau 0.25 MPa, qho so<120°C.

Cov Hlau Hlau
Siv rau media (dej, chav dej, huab cua, hydrogen, ammonia, nitrogen, roj av) ntawmPn tsawg dua los yog sib npaug rau 32.0 MPA, Kub: -30 Qib rau 425 Degree.
Cov qib kawm:WC1, WCB, ZG25, Hwm cov steels20, 25, 30, Thiab qis {- ecoy txheej txheem steel16mn.
Tooj liab alloy
Siv rau media (dej, seawater, oxygen, cua, roj) ntawmPn tsawg dua los yog sib npaug rau 2.5 MPA, ThiabChav rau -40 Qib rau 250 Qib.
Cov qib kawm:
Zgnsn10zn2(Tin bronze),
H62, HPB59-1(Tooj dag),
Qaz19-2, QA19-4(Txhuas Bronze).
High - kub steel
Siv rau cov khoom siv thiab cov khoom siv roj av ntawmPn tsawg dua los yog sib luag rau 17.0 MPA, kub tshaj lossis sib npaug rau 570 degree.
Cov qib kawm:
Zgcr5mo, 1cr5mo, zg20crmov, zg125cr1mo1v, 12crmov, WC6, WC9.
Cryogenic steel
Siv rau media (Ethylene, propylene, lng, kua nitrogen) ntawmPn tsawg dua los yog sib npaug rau 6.4 MPA, kub ntau dua los yog sib luag rau -196 degree.
Cov qib kawm:
ZG1CR18NI9,
0cr18ni9,
1Cr18NITI,
Zg0cr18ni9.

Stainless acid -} tiv taus hlau
Siv rau media (nitric acid, acetic acid) ntawmPn tsawg dua los yog sib npaug rau 6.4 MPA, kub tshaj lossis sib npaug rau 200 degree.
Cov qib kawm:
Zg0cr18ni99i,
Zg0cr18ni10
Zg0cr18ni12mo2ti,
Zg1cr18ni12mo2ti