A335 P92 American standard alloy seamless steel yeeb nkab yog siab -kub, siab -siab alloy seamless steel yeeb nkab tsim raws li American Society for Testing and Materials (ASTM) tus qauv. "A335" nyob rau hauv nws lub npe sawv cev rau cov series ntawm chromium-molybdenum alloy steel kav, thaum "P92" qhia cov khoom qib. Cov yeeb nkab steel no feem ntau yog ua los ntawm cov qib siab - zoo alloy steel, nrog rau cov khoom tseem ceeb xws li chromium, molybdenum, vanadium, niobium, thiab lwm yam. Los ntawm cov txheej txheem smelting thiab kev kho cua sov (xws li quenching thiab tempering), lub microstructure ruaj khov yog tsim, ua rau muaj kev kub siab zoo heev, oxidation tsis kam, thiab creep resistance.
Gnee Steel (Tianjin) Co., Ltd. yog ib qho ntawm feem txhim khu kev qha manufacturers thiab lwm tus neeg ntawm a335 p92 chrome moly alloy seamless yeeb nkab nyob rau hauv Tuam Tshoj, kuj txhawb customized kev pab cuam nrog luv nqi. Txais tos rau cov lag luam wholesale luv nqi a335 p92 chrome moly alloy seamless yeeb nkab rau muag ntawm no los ntawm peb lub hoobkas. Tiv tauj peb rau cov qauv dawb.
P92 belongs rau 9Cr-1Mo-V-Nb-W series ntawm martensitic thaum tshav kub kub-resistant steels, thiab yog siab- alloy khoom optimized thiab upgraded raws li P91 steel. Nws cov qauv tsim tseem hloov pauv ib feem ntawm molybdenum (Mo) nrog tungsten (W) thiab ntxiv cov lej ntawm boron (B) thiab niobium (Nb) los tsim cov theem ruaj khov nanoscale carbonitride ntxiv dag zog rau theem, txhim kho qhov kub thiab txias creep zog thiab oxidation tsis kam.
P92 seamless steel kav nruj me ntsis ua raws li ASTM A335 / A335M-23 (Specification for Ferritic Alloy Steel Seamless Pipes for High-Temperature Applications), xav tau kev kho cua sov dual ntawm normalizing thiab tempering los xyuas kom meej tias cov lath martensite cov ntsiab lus nyob rau hauv lub microstructure tsis sib npaug ntawm 9% thiab kev sib npaug kuaj xws li ultrasonic tsis pom kev thiab muaj CT imaging. Qee daim ntawv thov kuj yuav tsum ua raws li cov qauv hauv cheeb tsam xws li EN 10216-2 thiab GB / T 5310.
GNEE Group yog cov chaw tsim khoom thiab cov chaw muag khoom ntawm A335 P92 chromium-molybdenum alloy kav. Peb tau nruab nrog qhov tseeb eddy tam sim no kuaj thiab cov khoom siv ntsuas hydrostatic kom ntseeg tau qhov zoo ntawm txhua cov yeeb nkab. Cov ntaub ntawv pov thawj yog muab nrog txhua lub yeeb nkab thaum xa khoom.Tiv tauj pebrau siab -zoo A335 P92 siab-kub thiab siab- cov kav dej siab rau koj cov nroj tsuag fais fab, roj refineries, thiab cov nroj tsuag tshuaj.
A335 P92 High Pressure Boiler Yeeb Nkab Cov Tshuaj muaj pes tsawg leeg,%,
C: 0.07-0.13
Ntev: 0.30-0.60
P: Tsawg dua lossis sib npaug rau 0.020
S: Tsawg dua lossis sib npaug rau 0.010
Si: Tsawg dua lossis sib npaug li 0.50
8.50-9.50 Nws
Mo: 0.30-0.60 Nws
V: 0.15-0.25
N: 0.03-0.07
Ni: Tsawg dua lossis sib npaug li 0.40
Al: Tsawg dua lossis sib npaug rau 0.02
Cb: 0.04-0.09
W: 1.5-2.00
B: 0.001-0.006
Ti: Tsawg dua lossis sib npaug rau 0.01
Zr: Tsawg dua lossis sib npaug rau 0.01
A335 P92 Tsawg Alloy Seamless Round Pipes Kev kho cua sov yuav tsum tau ua
Normalizing (1040℃-1080 degree) ua raws li tempering (730℃-800 degree). Thaum cov phab ntsa thickness ntau dua 75 hli, txias ceev los ntawm qhov normalizing kub yuav tsum tau tso cai.
A335 P92 Chrome Moly boiler yeeb nkab Mechanical Property Requirements
Yield zog: Ntau dua lossis sib npaug rau 440MPa
Tensile Strength: Ntau dua lossis sib npaug rau 620MPa
A335 P92 Kub Kub Seamless Yeeb Nkab Elongation
| Qauv |
A335 P92 |
|
| Ntsug | Kab rov tav | |
| Yam tsawg kawg nkaus tus nqi ntawm cov qauv voj voog lossis me me - nplai cov qauv nrog lub ntsuas qhov ntev ntawm 4D. |
20 |
13 |
| Rectangular specimens nrog phab ntsa thickness ntawm 5/16 in. (7.94 mm) los yog ntau dua, thiab tag nrho cov me me -sized specimens ntawm tag nrho cov ntoo khaub lig-section, nrog ib tug gauge ntev ntawm 2 in. (50 mm). |
20 |
- |
| Rectangular specimens nrog phab ntsa tuab ntawm 5/16 in. (7.94 mm) lossis tsawg dua, nrog lub ntsuas qhov ntev ntawm 2 in. (50 mm) (specimen width 1/2 in., 12.7 mm). |
1.00A |
- |
A tso cai rau 1.0% txo nyob rau hauv longitudinal elongation rau txhua txhua 1/32 nyob rau hauv. (0.79 mm) txo nyob rau hauv phab ntsa thickness los ntawm cov saum toj no elongation nqi.
A335 P92 Chrome Moly Alloy Seamless Yeeb Nkab sab nraud txoj kab uas hla ntawm cov yeeb nkab steel
|
Sab nraud txoj kab uas hla D, mm |
Zoo kam rau ua, mm |
Negative kam rau ua, mm |
|
10.3-48.3 |
0.40 |
0.40 |
|
48.3<D Tsawg dua lossis sib npaug rau 114.3 |
0.79 |
0.79 |
|
114.3<D Tsawg dua lossis sib npaug rau 219.10 |
1.59 |
0.79 |
|
219.1<D Tsawg dua lossis sib npaug rau 323.9 |
2.38 |
0.79 |
|
>323.9 |
±1% D |
|
Hlau yeeb nkab phab ntsa thickness kam rau ua
|
Sab nraud txoj kab uas hla D, mm |
Kev kam rau siab,% |
Tsis zoo kam rau ua,% |
|
10.3-73 |
20.0 |
12.5 |
|
73, t / D Tsawg dua lossis sib npaug li 5% |
22.5 |
12.5 |
|
>73, t/D>5% |
15.0 |
12.5 |
t=qhia phab ntsa thickness, D=teev sab nraud
A335 P92 Chrome Moly Seamless Yeeb Nkab Daim Ntawv Thov
A335 P92 alloy yeeb nkab yog martensitic cua sov-cov hlau tsis muaj zog feem ntau siv hauv cov khoom siv tseem ceeb ua haujlwm nyob rau hauv siab - kub thiab siab - ib puag ncig siab. Cov ntawv thov ib txwm muaj xws li:
Kev lag luam fais fab
- Ultra-supercritical boilers: Siv rau cov kav dej tseem ceeb thiab rov ua cov kav dej, muaj peev xwm ua haujlwm ntev - lub sijhawm ruaj khov ntawm qhov kub siab tshaj 600℃.
- Nuclear Fais fab nroj tsuag: Siv los ua cov khoom siv rau cov khoom siv xws li cov khoom siv hluav taws xob sib hloov, tiv taus siab - kub, siab - siab, thiab hluav taws xob ib puag ncig.
Kev lag luam Petrochemical
- High -Tub Txheej Txheej Piping: Siv rau kev thauj khoom siab - kub thiab siab - siab reactants lossis chav, haum rau cov roj refineries, tshuaj nroj tsuag, thiab lwm qhov chaw zoo sib xws.
- Reactors thiab Heat Exchangers: Ua kom muaj kev nyab xeeb thiab kev ntseeg siab ntawm cov cuab yeej siv nyob rau hauv siab - kub thiab siab - cov txheej txheem siab.
A335 P92 High Pressure Alloy Steel Seamless Yeeb Nkab Hoobkas

A335 P92 Siab-Tub kub Alloy Steel Pipes Ntim thiab xa khoom

Cim npe nrov: a335 p92 chrome moly alloy seamless yeeb nkab, Tuam Tshoj a335 p92 chrome moly alloy seamless yeeb nkab manufacturers, lwm tus neeg, Hoobkas
Xa kev nug